MOLYKOTE BG-20

Harmonization Code : 8473.30.80.00 | Parts and accessories (other than covers, carrying cases and the like) suitable for use solely or principally with machines of headings 8470 to 8472 ; Parts and accessories of the machines of heading 8471 ; Other; Other

MOLYKOTE BG-20

Main features

  • DN 750,000 High-Speed Operation
  • Medium-to-Heavy Load Lubrication
  • -45 to 180 deg C Service

Product Description

MOLYKOTE BG-20 Synthetic Bearing Grease is a polyolester-based, lithium-complex grease for metal-to-metal bearing contacts under medium to heavy loads and high to very high speeds. It has a base-oil viscosity of 55 mm2/s at 40 deg C and a service range of -45 to 180 deg C, with short exposures up to 200 deg C. The grease supports a DN value of 750,000 and is applied by brush, spatula, grease gun, automatic lubricator, or central lubrication system. Typical uses include clutch release, blower, calender-roller, and electric motor bearings.

Key features

  • DN 750,000 Speed Capability: Supports high to very high rotational speeds at a DN value of 750,000.
  • Medium-to-Heavy Load Lubrication: Four-ball weld load is 2,400 N and Almen-Wieland OK load is 20,000 N.
  • Wide Service-Temperature Range: Operates from -45 to 180 deg C, with short periods up to 200 deg C.

Applications / Suitable for

  • Clutch release, blower, calender-roller, and electric motor bearings.
  • Machining spindles and rolling-element bearings.
  • Power screw drives.
  • Slides, guides, and tracks.
Product Family

MOLYKOTE BG-20

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Beige
Density (g)
1.01 g/cm3
Thermal Properties
Service temperature
-45 to 180 °C

Additional Information

Technical properties

Grease properties

Property Value Unit Method / condition
Unworked penetration 240 to 270 mm/10 ISO 2137; typical
Density 1.01 g/ml ISO 2811 at 20 deg C; typical
Base-oil viscosity 55 mm2/s DIN 51562 at 40 deg C; typical
Drop point >295 deg C ISO 2176; test result, not a service-temperature limit
Technical properties

In-service performance properties

Property Value Unit Method / condition
Service-temperature range -45 to 180 deg C Short periods up to 200 deg C
Four-ball weld load 2,400 N DIN 51350, Part 4; typical
Four-ball wear scar 1.0 mm DIN 51350, Part 5 under 800 N load; typical
Almen-Wieland OK load 20,000 N Typical
FE9 bearing test life 662 h DIN 51821-02A, 1,500/6,000/160 deg C; average
DN value 750,000 mm/min Calculated approximation; varies with temperature, load, and bearing type
Corrosion degree 1 to 2 DIN 51802, SKF-Emcor method; typical
Oil separation 1.2 % DIN 51817 standard test; typical