LORD SC-1600

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

LORD SC-1600

Main features

  • 3.7 W/(m K) Conductivity
  • Equal 1:1 Meter-Mix Processing
  • 30-Minute Heat Cure

Product Description

CoolTherm SC-1600 Thermally Conductive Silicone Gap Filler is a two-component, addition-curing silicone thermal interface material for filling gaps in electronic assemblies. The resin and hardener mix 1:1 by weight or volume and can be dispensed from cartridges or automatic meter/mix equipment. The mixed light-pink paste has a typical specific gravity of 3.3 and a 60 minute tack-free working time at 25 deg C. It cures in 24 hours at 25 deg C or 30 minutes at 100 deg C and develops a typical thermal conductivity of 3.7 W/(m K), Shore OO 89 hardness, and 25% elongation.

Key features

  • 3.7 W/(m K) Conductivity: Provides typical bulk thermal conductivity after cure.
  • Equal 1:1 Mixing: Uses a 1:1 resin-to-hardener ratio by weight or volume.
  • Room-Temperature or Heat Cure: Cures in 24 hours at 25 deg C or 30 minutes at 100 deg C.

Applications / Suitable for

  • Thermally conductive gap filling in electronic assemblies.
Product Family

LORD SC-1600

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Resin: Pink Paste | Hardener: White to Gray Paste | Mixed: Light Pink Paste
Specific Gravity
A/B/Mixed: 3.3
Physical Properties
Viscosity (Part A)
1/s Resin: 318000 mPa.s
Viscosity (Part B)
1/s Hardener: 205000 mPa.s

Additional Information

Technical properties

Component and mixed-system properties

Component and mixed-system values are typical.

Property Value Unit Method / condition
Resin appearance Pink paste As supplied; typical
Hardener appearance White to gray paste As supplied; typical
Mixed appearance Light pink paste Mixed 1:1; typical
Resin viscosity 318,000 at 1/s; 114,000 at 10/s mPa s 25 deg C; typical
Hardener viscosity 205,000 at 1/s; 75,000 at 10/s mPa s 25 deg C; typical
Specific gravity 3.3 Resin, hardener, and mixed system; typical
Mix ratio 1:1 by weight or volume Resin : hardener
Tack-free working time 60 min 25 deg C; mixed system; typical
Technical properties

Cured gap-filler properties

Values apply to the cured SC-1600 gap filler.

Property Value Unit Method / condition
Cure schedule 24 h at 25 deg C or 30 min at 100 deg C Time begins after the material reaches target temperature
Thermal conductivity 3.7 W/(m K) ISO 22007-2, Hot Disc transient method; typical
Hardness 89 Shore OO ASTM D2240; typical
Tensile strength 0.47 MPa ASTM D638; typical
Elongation at break 25 % ASTM D638; typical
Elastic modulus 3.1 MPa ASTM D638; typical
Dielectric strength 12.1 kVDC/mm; 7.6 kVAC/mm ASTM D149, 0.8 mm specimen; typical