LORD P-1291

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

LORD P-1291

Main features

  • Low-Viscosity Brush or Spray
  • Metal and Glass Adhesion Promotion
  • 30 to 60 Minute Air-Dry

Product Description

LORD P-1291 Primer is a low-viscosity, one-component adhesion primer for promoting bonds between tin-catalyzed RTV silicone rubbers and most metals or glass. It may also be used with some addition-cure silicone systems. The clear liquid can be brushed or sprayed onto properly cleaned surfaces, with a recommended 12 to 25 micron film and a 30 to 60 minute air-dry period before silicone application. Typical as-supplied values include 5 cP viscosity and 0.85 specific gravity at 25 deg C. The exact color variant of this generic primer requires confirmation.

Key features

  • Low-viscosity brush or spray: The 5 cP clear liquid supports controlled primer application by brush or spray.
  • Metal and glass adhesion promotion: Promotes bonding of tin-catalyzed RTV silicone rubber to most metals and glass in the supported applications.
  • 30 to 60 minute air-dry: Provides a defined ambient drying step before the supported RTV silicone is applied.

Applications

Applications include promoting adhesion of tin-catalyzed RTV silicone rubbers to most metals and glass, with possible use in some addition-cure silicone systems.

Product Family

LORD P-1291

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Clear Liquid
Specific Gravity
0.85
Physical Properties
Viscosity
5 mPa.s
Thermal Properties
Flash Point
-8.33 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied values apply to the generic LORD P-1291 Primer entity; the source-row color variant is not confirmed.

PropertyValueUnitMethod / condition
AppearanceClear liquid-Typical; as supplied
Viscosity5cPTypical at 25 deg C
Specific gravity0.85-Typical at 25 deg C
Flash point-8.33deg CTypical; source method not stated
Shelf life1yearOriginal unopened container in a cool, dry environment at 15 to 35 deg C