LORD MAXLOK MX/T3S

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

LORD MAXLOK MX/T3S

Main features

  • Minimal-Preparation Metal Bonding
  • Fast 6- to 8-Minute Handling
  • Controlled Non-Sag Bondline

Product Description

LORD Maxlok MX/T3S is a two-part acrylic adhesive system that combines T3S adhesive with MX accelerator for bonding a wide range of metals with minimal surface preparation. Mixed at 1:4 adhesive-to-accelerator by volume, the system provides a 3 to 5 minute working time and reaches 50 psi shear handling strength in 6 to 8 minutes at 25 deg C. Its non-sag consistency supports vertical and overhead application, while 0.010 in (0.025 cm) glass beads help control bondline thickness. After cure, the adhesive performs from -40 to 149 deg C and resists moisture, salt spray, weathering, oils, solvents, dilute acids, alkalis, and indirect UV exposure.

Key features

  • Rapid handling strength: Reaches 50 psi shear handling strength in 6 to 8 minutes at 25 deg C after a 3 to 5 minute working time.
  • Controlled non-sag application: Remains in position on vertical and overhead surfaces, with glass beads for 0.010 in bondline control.
  • Wide-temperature resistance: Performs from -40 to 149 deg C with resistance to moisture, salt spray, weathering, and indirect UV exposure.

Applications

Replacing welding, brazing, riveting, and other mechanical fastening methods in assemblies exposed to high impact, high peel loads, or broad temperature environments.

Product Family

LORD MAXLOK MX/T3S

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Off-white to Tan Paste
Density
989 -1048 kg/m3
Physical Properties
Viscosity
70,000 - 200,000 mPa.s
Thermal Properties
Flash Point
15 °C

Additional Information

Technical properties

As-Supplied / Before-Processing Properties

Values are typical and not for specification purposes. T3S adhesive, MX accelerator, and mixed-system properties are identified separately.

Property Value Unit Method / condition
T3S adhesive appearance Off-white to tan paste - As supplied
T3S adhesive viscosity 70,000 to 200,000 cP Brookfield at 77 deg F (25 deg C)
T3S adhesive density 8.25 to 8.75 lb/gal 989 to 1048 kg/m^3
MX accelerator appearance Grey paste - As supplied
MX accelerator viscosity 100,000 to 500,000 cP Brookfield at 77 deg F (25 deg C)
MX accelerator density 11.45 to 12.15 lb/gal 1372 to 1456 kg/m^3
Mix ratio 1:4 Adhesive:accelerator By volume
Solids content 100 % Adhesive mixed with recommended accelerator
Technical properties

After-Processing / Final-State Properties

MX/T3S processing values are typical. Service and resistance characteristics are stated for the Maxlok MX/T3S, MX/T6S, and MX/T18S series.

Property Value Unit Method / condition
Time to handling strength 6 to 8 min At 77 deg F (25 deg C); 50 psi shear
Complete cure 24 h At room temperature; mating surfaces held in contact during cure
Service temperature range -40 to 149 deg C Cured adhesive; equivalent source range -40 to 300 deg F
Bondline control 0.010 in Glass bead diameter; 0.025 cm
Environmental resistance Dilute acids, alkalis, solvents, greases, oils, moisture, salt spray, and weathering Qualitative Cured adhesive
Indirect UV resistance Excellent Qualitative Cured adhesive under indirect UV exposure