LORD 850S/25GB

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LORD 850S/25GB

Main features

  • Welding/Fastener Replacement Bonding
  • 6 to 10-Minute Working Time
  • Documented Chemical/Moisture/Salt-Spray/Weather Resistance

Product Description

LORD® 850S/25GB Toughened Structural Acrylic Adhesive is a two-component structural acrylic adhesive system consisting of LORD® 850S Adhesive and LORD® Accelerator 25GB. Designed to replace welding, brazing, riveting and other mechanical fastening methods, it bonds a wide variety of prepared and unprepared metals as well as selected engineered plastics and polymer composite substrates. The toughened formulation provides excellent impact and peel strength while accommodating demanding structural bonding applications.

Key Features

  • Replaces welding, brazing, riveting and other mechanical fastening methods.
  • Bonds prepared and unprepared metals, FRP and selected engineered plastics with minimal substrate preparation.
  • High impact and peel strength with 100% elongation for improved fatigue resistance.
  • Service temperature from -40°F to +300°F (-40°C to +149°C).
  • Non-sag formulation for vertical and overhead applications.
  • Resists dilute acids, alkalis, solvents, greases, oils, moisture, salt spray, weathering and indirect UV exposure.

Suitable For

  • Structural metal bonding
  • FRP and composite bonding
  • Engineered plastic bonding
  • Automotive assembly applications
  • Industrial structural assembly
Product Family

LORD 850S/25GB

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Amber Paste
Density
959-995 kg/m3
Physical Properties
Viscosity
150000-550000 mPa.s
Thermal Properties
Flash Point
59 °C

Additional Information

As-Supplied / Before-Processing Properties

Property Value
Appearance Amber paste
Viscosity 150,000–550,000 cP @ 77°F (25°C), Brookfield
Density 8.00–8.30 lb/gal (959–995 kg/m³)
Flash Point 59°F (15°C), Seta Closed Cup
Mix Ratio 10:1 by volume (Adhesive : LORD® Accelerator 25GB)
Mixed Appearance Red paste
Working Time 6–10 minutes @ 75°F (24°C)
Time to Handling Strength 18–24 minutes @ 75°F (24°C), 50 psi shear
Full Cure Time 2 hours @ 75°F (24°C) (90% strength after 1 hour)
Solids Content 100%

After-Processing / Final-State Properties

Property Value Test Method
Hardness Shore D 66 —
Tensile Strength at Break 2,610 psi (18.0 MPa) ASTM D638, modified
Elongation 100% ASTM D638, modified
Young's Modulus 105,000 psi (724 MPa) ASTM D638, modified
Glass Transition Temperature (Tg) 176°F (80°C) ASTM E1640-99 (DMA)

Leading Brands Trust in Our Products and Services