LORD 7800

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

LORD 7800

Main features

  • Rapid-Cure Urethane Bonding
  • Composite, SMC, Plastic, and Coated-Metal Bonding
  • Non-Sag Environmental Resistance

Product Description

LORD® 7800 Fast Cure Urethane Adhesive is an equal-mix, two-component urethane adhesive system designed for bonding composites, sheet molding compound (SMC), plastics and coated metals with minimal surface preparation. The system provides rapid strength development while offering multiple curative options that maintain consistent mechanical and adhesion properties across different working times, making it suitable for a wide range of manufacturing processes. It is also qualified under GMW 16506 Exterior Lighting Structural Adhesives for automotive and truck headlamp assembly.

Key Features

  • Equal-mix, two-component urethane adhesive system.
  • Rapid cure strength to support faster manufacturing and processing.
  • Low exotherm cure for more consistent cure speed across bondline thicknesses.
  • Non-sag formulation for vertical and overhead applications.
  • Resists weathering, humidity and salt spray after cure.
  • Free of heavy metals and does not contain ozone-depleting chemicals.

Suitable For

  • Composite bonding
  • Sheet Molding Compound (SMC) bonding
  • Plastic bonding
  • Powder-coated, primed and E-coat metal bonding
  • Automotive and truck headlamp assemblies
Product Family

LORD 7800

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Mix Ratio
7800 A/C: 1:1 | 7800 A/D: 1:1
Solids
A/C | A/D : 100/100 %
Mechanical Properties
Elongation
130 %
Thermal Properties
Glass Transition Temperature (Tg)
47 °C

Additional Information

As-Supplied / Before-Processing Properties

Property 7800-A Resin 7800-C Curative 7800-D Curative
Appearance Black liquid Tan liquid Tan liquid
Viscosity @ 77°F (25°C) 8,000–25,000 cP 33,000–60,000 cP 33,000–60,000 cP
Density 10.7–11.85 lb/gal (1282–1420 kg/m³) 10.0–10.7 lb/gal (1198–1282 kg/m³) 10.0–10.7 lb/gal (1198–1282 kg/m³)
Flash Point (Closed Cup) >200°F (>93°C) >200°F (>93°C) >200°F (>93°C)
Mix Ratio (Resin:Curative) 1:1 by volume
Solids Content 100 wt%
Working Time @ 75°F (24°C) 2–4 minutes (7800-A/C) 5–7 minutes (7800-A/D)
Time to Handling Strength @ 75°F (24°C) 12 minutes (7800-A/C) 15 minutes (7800-A/D)

After-Processing / Final-State Properties

Property Value Test Method
Hardness Shore D 60 —
Tensile Strength at Break 3000 psi (20.7 MPa) ASTM D638, modified
Elongation 130% ASTM D638, modified
Young's Modulus 25,000 psi (172 MPa) ASTM D638, modified
Glass Transition Temperature (Tg) 117°F (47°C) ASTM E1640-99 (DMA)