LORD 7550C Urethane Adhesive

Harmonization Code : 3907.30.00.15 | Epoxide resin, halogen-free

LORD 7550C Urethane Adhesive

Main features

  • Equal-Mix LORD 7550 Curative Component
  • 6,000 to 12,500 cP Viscosity
  • Lexan, ABS, and Primed-Metal Bonding

Product Description

LORD® 7550C Urethane Adhesive Curative is the curative component of the equal-mix LORD 7550 two-component clear urethane adhesive system. When combined 1:1 by volume with LORD 7550A resin, the system bonds Lexan, ABS, polycarbonate, other plastics, and properly prepared and primed metals. The clear-to-yellow liquid curative has a typical viscosity of 6,000 to 12,500 cP at 25°C. The mixed adhesive is self-leveling, has a typical working time of three to five minutes, reaches handling strength in approximately 60 minutes, and cures to full strength in about 72 hours at room temperature.

Key features

  • LORD 7550 curative component: LORD 7550C is mixed 1:1 by volume with LORD 7550A resin.
  • Controlled liquid viscosity: Typical component viscosity is 6,000 to 12,500 cP at 25°C.
  • Clear urethane bonding system: The paired system is documented for plastics and properly prepared and primed metals.

Applications / Suitable for

  • Curative component of the LORD 7550 urethane adhesive system
  • Bonding Lexan, ABS, polycarbonate, and other plastics
  • Bonding properly prepared and primed metals
Product Family

LORD 7550C

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Clear to Clear Yellow Liquid
Density
1078 -1126 kg/m3
Physical Properties
Viscosity
6000 -12,500 mPa.s
Thermal Properties
Flash Point
>93 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or mixed-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Component role Curative N/A LORD 7550C
Appearance Clear to clear-yellow liquid N/A As supplied
Viscosity 6,000 to 12,500 cP At 25°C
Density 1,078 to 1,126 kg/m³ As supplied
Flash point >93 °C Closed cup
Shelf life 6 months At 21°C to 27°C in the original unopened container