LORD 7550A Urethane Adhesive

Harmonization Code : 3907.30.00.15 | Epoxide resin, halogen-free

LORD 7550A Urethane Adhesive

Main features

  • Equal-Mix LORD 7550 Resin Component
  • 1,800 to 4,000 cP Viscosity
  • Lexan, ABS, and Primed-Metal Bonding

Product Description

LORD® 7550A Urethane Adhesive Resin is the resin component of the equal-mix LORD 7550 two-component clear urethane adhesive system. When combined 1:1 by volume with LORD 7550C curative, the system bonds Lexan, ABS, polycarbonate, other plastics, and properly prepared and primed metals. The clear-to-yellow liquid resin has a typical viscosity of 1,800 to 4,000 cP at 25°C. The mixed adhesive is self-leveling, has a typical working time of three to five minutes, reaches handling strength in approximately 60 minutes, and cures to full strength in about 72 hours at room temperature.

Key features

  • LORD 7550 resin component: LORD 7550A is mixed 1:1 by volume with LORD 7550C curative.
  • Low-viscosity liquid resin: Typical component viscosity is 1,800 to 4,000 cP at 25°C.
  • Clear urethane bonding system: The paired system is documented for plastics and properly prepared and primed metals.

Applications / Suitable for

  • Resin component of the LORD 7550 urethane adhesive system
  • Bonding Lexan, ABS, polycarbonate, and other plastics
  • Bonding properly prepared and primed metals
Product Family

LORD 7550A

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Clear to Clear Yellow Liquid
Density
1150 -1174 kg/m3
Physical Properties
Viscosity
1800 - 4000 mPa.s
Thermal Properties
Flash Point
>93 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or mixed-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Component role Resin N/A LORD 7550A
Appearance Clear to clear-yellow liquid N/A As supplied
Viscosity 1,800 to 4,000 cP At 25°C
Density 1,150 to 1,174 kg/m³ As supplied
Flash point >93 °C Closed cup
Shelf life 6 months At 21°C to 27°C in the original unopened container