LORD 7150A/B

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

LORD 7150A/B

Main features

  • High-Strength Structural Bonding
  • Primerless Bonding to Many Plastics
  • Solvent-, Weathering- and Aging-Resistant Gray Cured System

Product Description

LORD® 7150-A/B Urethane Adhesive is a two-part, high-strength urethane adhesive used to bond cloth, paper, plastics, foams, rubber, painted metals and powder-coated metals. The system combines an isocyanate-based LORD® 7150-A resin with a polyol-based LORD® 7150-B curative and can be cured at room temperature or with elevated heat for faster processing. After cure, it forms a gray adhesive system with resistance to solvents, weathering and aging.

Key Features

  • Broad substrate capability for cloth, paper, plastics, foams, rubber, painted metals and powder-coated metals.
  • High-strength plastic bonding without crazing, attacking or reducing the strength of the plastic substrate.
  • Reduced priming requirements for many plastics, helping lower material and labor requirements.
  • Solvent-, weathering- and aging-resistant cured performance with no VOC content and no ozone-depleting chemicals.

Applications / Suitable for

  • Plastic and foam assemblies
  • Rubber bonding
  • Cloth and paper laminations
  • Painted-metal and powder-coated-metal assemblies
Product Family

LORD 7150A/B

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
A (Resin)/ B(Curative): Black/White Liquid
Density
A (Resin): 1486 -1522 | B(Curative): 1306 -1366 kg/m3
Physical Properties
Viscosity
A (Resin): 3000 -16,000 | B (Curative): 41,500 - 65,500 mPa.s
Thermal Properties
Flash Point
A (Resin)/ B(Curative): >93 °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Typical component and mixed-system properties for LORD® 7150-A/B Urethane Adhesive. Values are typical and are not intended for specification purposes.

Property 7150-A Resin 7150-B Curative Mixed System Method / Condition
Composition Isocyanate-based resin Polyol-based curative Two-part urethane Product description
Appearance Black liquid White liquid — Typical
Viscosity 3,000–16,000 cP 41,500–65,500 cP — At 77°F (25°C); resin: Brookfield LVT, Spindle 4, 30 rpm; curative: Brookfield HA, Spindle 6, 20 rpm
Density 12.4–12.7 lb/gal
(1486–1522 kg/m³)
10.9–11.4 lb/gal
(1306–1366 kg/m³)
— Typical
Flash Point >200°F
(>93°C)
>200°F
(>93°C)
— Closed cup
Mix Ratio 1 part 2 parts by volume
1.78 parts by weight
1:2 by volume
1:1.78 by weight
Resin to curative
Solids Content — — 100% Mixed adhesive
Working Time — — 5–10 minutes At 75°F (24°C)
Purge Time — — 3 minutes At 77°F (25°C)
Time to Handling Strength — — 2–3 hours At 73°F (23°C)
Shelf Life 6 months 6 months — Store at 65–85°F (18–30°C) in a clean, dry environment in the original, unopened container
Technical Properties

After-Processing / Final-State Properties

Supported cure and final-state characteristics for LORD® 7150-A/B Urethane Adhesive. Values are typical and are not intended for specification purposes.

Property Value Unit Method / Condition
Full Cure Time 24 hours At room temperature, 77°F (25°C); elevated temperatures accelerate cure
Cured Appearance Gray — Typical
VOC Content 0 g/L Documented formulation characteristic