LORD 459X

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

LORD 459X

Main features

  • Adhesion-Promoting Surface Treatment
  • Low-Viscosity Adhesive Application
  • Brush, Dip or Spray Application

Product Description

LORD® 459X Adhesion Enhancer/Surface Modifier is a low-viscosity, xylene-based surface treatment designed to promote adhesion to difficult-to-bond thermoplastic elastomers, thermoplastic polyolefins and EPDM. Supplied pre-diluted for direct application, it can be used with LORD acrylic, urethane and epoxy structural adhesives, as well as compatible coatings and double-sided tapes. The material requires no mixing or additional dilution and can be applied by brush, dip or spray.

Key Features

  • Promotes adhesion to difficult elastomers, including TPE, TPO and EPDM substrates.
  • Ready-to-use formulation requires no mixing or dilution before application.
  • Low-viscosity application supports brush, dip and spray methods.
  • Low dry-film requirement with an optimum dry-film thickness of approximately 0.1 mil (2.5 µm).

Applications / Suitable for

  • Surface treatment of TPE, TPO and EPDM
  • Adhesion promotion for acrylic, urethane and epoxy structural adhesives
  • Adhesion enhancement for coatings
  • Surface preparation for compatible double-sided tapes
Product Family

LORD 459X

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Amber Liquid
Density
857-881 kg/m3
Physical Properties
Viscosity
10 mPa.s
Thermal Properties
Flash Point
27 °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Typical as-supplied properties. Values are typical and are not intended for specification purposes.

Property Value Unit Method / Condition
Appearance Amber liquid — Typical
Viscosity Approximately 10 cP Brookfield LVT, Spindle 1, 60 rpm at 77°F (25°C)
Density 7.15–7.35
(857–881)
lb/gal
(kg/m³)
Typical
Solids Content by Weight 2.7–4.1 % Typical
Flash Point 81
(27)
°F
(°C)
Seta
Solvent Xylene — Supplied pre-diluted for direct application
Mixing Requirement None — No mixing or dilution required
Shelf Life 6 months From date of shipment; store at 70–80°F (21–27°C) in the original, unopened container
Technical Properties

After-Processing / Final-State Properties

Supported applied-film and drying conditions for LORD® 459X Adhesion Enhancer/Surface Modifier.

Property Value Unit Method / Condition
Optimum Dry-Film Thickness Approximately 0.1
(2.5)
mil
(µm)
Applied by brush, dip or spray
Room-Temperature Air-Dry Time 30–60 minutes Room temperature with good airflow
Oven-Dry Schedule 5–10 minutes At 200–250°F (93–121°C); heat cycling generally improves adhesion