LORD 406E

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

LORD 406E

Main features

  • High-Impact and Peel Performance
  • 6-10 Minute Working Time
  • Minimal Metal Surface Preparation

Product Description

LORD 406E Acrylic Adhesive is a non-sag acrylic adhesive component used with LORD Accelerator 17, 19, or 19GB for structural bonding of metals and engineered plastics. The off-white to tan paste has a typical viscosity of 100,000 to 300,000 mPa s at 25 deg C and remains in position on vertical or overhead surfaces. With a recommended accelerator, the mixed system provides a 6 to 10 minute working time, 12 to 17 minute handling-strength time, and 24 hour full cure at 24 deg C. The cured system is formulated for high-impact and high-peel applications from -40 to 149 deg C.

Key features

  • High-Impact Acrylic Bonding: Supports bonded assemblies exposed to impact and peel loading.
  • 6-10 Minute Working Time: Provides a controlled assembly window when mixed with a recommended accelerator.
  • Non-Sag Application: Remains in position on vertical and overhead surfaces.

Applications

Applications include structural bonding of prepared or minimally prepared metals and engineered plastics in assemblies requiring impact or peel resistance.

Product Family

LORD 406E

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Off-White to Tan Paste
Density
1090 -1162 kg/m3
Thermal Properties
Flash Point
14 °C
Physical Properties
Viscosity
100000 to 300000 mPa.s

Additional Information

Technical properties

Adhesive component properties

Accelerator selection changes the required mix ratio and the applicable cured-property set.

Property Value Unit Method / condition
Appearance Off-white to tan paste As supplied
Viscosity 100,000 to 300,000 mPa s 25 deg C, Brookfield
Density 9.10 to 9.70 lb/gal 25 deg C
Flash point 15 deg C Closed-cup value
Mix ratio with Accelerator 17 10:1 by volume Adhesive : accelerator
Mix ratio with Accelerator 19 or 19GB 4:1 by volume Adhesive : accelerator
Technical properties

Mixed and cured adhesive properties

Cured mechanical values shown here apply to LORD 406 with Accelerator 19 under the documented test conditions.

Property Value Unit Method / condition
Working time 6 to 10 min 24 deg C, mixed with a recommended accelerator
Handling-strength time 12 to 17 min 24 deg C, 0.41 MPa shear criterion
Full-cure time 24 h 24 deg C
Tensile strength 18.6 MPa Cured with Accelerator 19
Elongation at break 30 % Cured with Accelerator 19
Glass transition temperature 72 deg C Cured with Accelerator 19
Service temperature range -40 to 149 deg C Complete adhesive system