LORD 403

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LORD 403

Main features

  • LORD Accelerator 17/19/19GB Compatibility
  • Alternative to Welding/Brazing/Fastening
  • Acrylic Adhesive with Multiple Accelerators

Product Description

LORD® 403 Acrylic Adhesive is an acrylic adhesive designed for use with LORD Accelerator 17, 19 or 19GB. When used as a complete adhesive system, it provides an alternative to welding, brazing, riveting and other mechanical fastening methods. Product-specific selection must account for the chosen accelerator because working time, cure behavior and final performance may vary by system configuration.

Key Features

  • Compatible with LORD Accelerator 17, 19 or 19GB as supported system options.
  • Alternative to mechanical fastening methods including welding, brazing and riveting.
  • Two-component acrylic adhesive system requiring the appropriate accelerator for use.
Product Family

LORD 403

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Off-White to Tan Paste
Density
1144 kg/m3
Thermal Properties
Flash Point
15 °C
Physical Properties
Viscosity
100000 to 300000 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Typical component and mixed-system properties for LORD® 403 Acrylic Adhesive used with LORD® Accelerator 19 Black. Values are typical and are not intended for specification purposes.

Property LORD 403 Adhesive Accelerator 19 Black Mixed System Method / Condition
Appearance Off-white to tan paste Black/gray paste Gray paste Typical
Viscosity 100,000–300,000 cP ≥250,000 mPa·s — LORD 403: Brookfield at 77°F (25°C); Accelerator 19 Black: 25°C
Density 9.25–9.55 lb/gal
(1108–1144 kg/m³)
12.55 lb/gal
(1.51 g/cm³)
— Typical
Flash Point 59°F
(15°C)
≥201°F
(≥93°C)
— Setaflash closed cup
Mix Ratio 4 parts by volume
3.00 parts by weight
1 part 4:1 by volume
3.00:1 by weight
Adhesive to Accelerator 19 Black
Solids Content — — 100% Mixed adhesive system
Working Time — — 2–4 minutes At 75°F (24°C)
Time to Handling Strength — — 4–6 minutes At 75°F (24°C); 50 psi shear
Typical Shelf Life 9 months — — Below 80°F (27°C) in original, unopened container; storage at 40–50°F (4–10°C) recommended
Technical Properties

After-Processing / Final-State Properties

Typical cured properties for LORD® 403 Acrylic Adhesive mixed with LORD® Accelerator 19. Values are typical and are not intended for specification purposes.

Property Value Unit Method / Condition
Full Cure Time 24 hours At 75°F (24°C); approximately 90% of full strength after 2 hours
Cured Appearance Black — With Accelerator 19 Black
Tensile Strength at Break 2700
(18.6)
psi
(MPa)
ASTM D638, modified; LORD 403 with Accelerator 19
Elongation 30 % ASTM D638, modified; LORD 403 with Accelerator 19
Young’s Modulus 130,000
(896.3)
psi
(MPa)
ASTM D638, modified; LORD 403 with Accelerator 19
Glass Transition Temperature 162
(72)
°F
(°C)
ASTM E1640-99, by DMA; LORD 403 with Accelerator 19
Temperature Range -40 to 300
(-40 to 149)
°F
(°C)
Documented product-family performance range