LORD 306-1

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LORD 306-1

Main features

  • High-Viscosity Non-Sag Gap Filling
  • Documented Chemical/Moisture/Weather Resistance
  • MIL-A-24456 Compliance Scope

Product Description

LORD® 306-1/306-2 Epoxy Adhesive is a general-purpose, high-viscosity, two-component epoxy adhesive formulated for structural bonding applications requiring excellent gap-filling capability and non-sag performance on vertical or overhead surfaces. The adhesive system provides durable, chemically and environmentally resistant bonds and conforms to MIL-A-24456 for bonding plastic vibration damping tiles to steel. It can be cured at room temperature or heat cured for faster production while delivering reliable service across temperatures from -30°F to +250°F (-34°C to +121°C). :contentReference[oaicite:0]{index=0}

Key Features

  • High-viscosity, non-sag epoxy formulation for gap filling and vertical or overhead applications.
  • Provides durable structural bonds with resistance to moisture, weathering, dilute acids, alkalis, solvents, greases and oils.
  • Low-shrinkage adhesive with good creep resistance and low water absorption for demanding industrial assemblies.

Applications / Suitable for

  • General structural bonding applications
  • Gap-filling and non-sag bonding on vertical or overhead surfaces
  • Bonding plastic vibration damping tiles to steel
  • Industrial metal and engineering material assemblies
Product Family

LORD 306-1

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
306-1 Resin: Grey Paste | 306-2 Hardener: Off White Paste
Density
Resin: 1378 -1474 | Hardener: 1007-1078 kg/m3
Physical Properties
Viscosity
Resin: 40,000 - 400,000 | Hardener: 20,000 - 100,000 mPa.s
Thermal Properties
Flash Point
Resin: 85 | Hardener: >93 °C

Additional Information

As-Supplied / Before-Processing Properties

Property 306-1 Resin 306-2 Hardener Method / Condition
Appearance Grey Paste Off-white Paste Typical
Viscosity 40,000–400,000 P 20,000–100,000 P Brookfield HBF, Helipath, 1 rpm (T-Bar Spindle E / C), 77°F (25°C)
Density 11.5–12.3 lb/gal (1378–1474 kg/m³) 8.4–9.0 lb/gal (1007–1078 kg/m³) Typical
Flash Point 185°F (85°C) >200°F (>93°C) Closed Cup
General Purpose Mix Ratio 1:1.3 by volume (1:1 by weight) -30°F to +250°F (-34°C to +121°C)
MIL-A-24456 Mix Ratio 5:3 by weight Specification
Solids Content 100% Mixed adhesive
Working Time 1–2 hours 75°F (24°C), 54 g mass
Time to Handling Strength 8–16 hours Temperature dependent
Mixed Appearance Grey Paste Typical
Shelf Life 2 years Stored unopened at 60–80°F (16–27°C)

After-Processing / Final-State Properties

Property Value Method / Condition
Cure Schedule 24–48 hours 65°F (18°C) or higher
Service Temperature -30°F to +250°F (-34°C to +121°C) Typical operating range
Tensile Strength at Break 4360 psi (30.1 MPa) ASTM D882-83A (modified)
Elongation 10% ASTM D882-83A (modified)
Young's Modulus 146,070 psi (1007 MPa) ASTM D882-83A (modified)
Glass Transition Temperature (Tg) 133°F (56°C) ASTM E1640-99 by DMA
Cured Appearance Grey Typical