LORD 305-1

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LORD 305-1

Main features

  • Medium-Viscosity Application Control
  • Rubber-to-Wood Epoxy Bonding
  • Chemically, Environmentally and Temperature Resistant

Product Description

LORD® 305-1/305-2 Epoxy Adhesive is a general-purpose, medium-viscosity, two-component epoxy adhesive designed to produce strong, durable, chemically and environmentally resistant structural bonds. It provides excellent adhesion to prepared metals, fiberglass reinforced plastics (FRP), phenolics, wood, prepared rubber and other engineering materials. The adhesive is also suitable for bonding cured rubber to itself and rubber to metal, including gaskets, bushings, shock-absorbing devices and rubber rolls. LORD® 305 can be cured at room temperature or heat cured to accelerate production while delivering reliable performance across a service temperature range of -30°F to +250°F (-34°C to +121°C). :contentReference[oaicite:0]{index=0}

Key Features

  • Medium-viscosity, two-component epoxy adhesive for durable structural bonding.
  • Excellent adhesion to metals, FRP, phenolics, wood, prepared rubber and other engineering substrates.
  • Resists moisture, sunlight, weathering, dilute acids, alkalis, solvents, greases and oils while providing low shrinkage and good creep resistance.

Applications / Suitable For

  • General structural bonding applications
  • Metal and composite assemblies
  • Bonding cured rubber to itself or to metal components
  • Gaskets, bushings, shock-absorbing devices and rubber rolls
Product Family

LORD 305-1

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
305-1 Resin: Clear Amber Liq | 305-2 Hardener: Blue Liq
Density
Resin: 1126 -1198 | Hardener: 928 -1001 kg/m3
Physical Properties
Viscosity
Resin: 10,000 -18,000 | Hardener: 20,000 - 45,000 mPa.s
Thermal Properties
Flash Point
Resin: >93 | Hardener: >93 °C

Additional Information

As-Supplied / Before-Processing Properties

Property 305-1 Resin 305-2 Hardener Method / Condition
Appearance Clear amber liquid Blue liquid Typical
Viscosity 10,000–18,000 cP 20,000–45,000 cP Brookfield HBF, Spindle 2, 10 rpm, 77°F (25°C)
Density 9.4–10.0 lb/gal (1126–1198 kg/m³) 7.75–8.35 lb/gal (928–1001 kg/m³) Typical
Flash Point >200°F (>93°C) >200°F (>93°C) Closed Cup
General Purpose Mix Ratio 1:1 by volume (1.2:1 by weight) -30°F to +250°F (-34°C to +121°C)
Solids Content 100% Mixed adhesive
Working Time 1–2 hours 75°F (24°C), 54 g mass
Time to Handling Strength 8–16 hours Typical
Mixed Appearance Blue liquid Typical
Shelf Life 2 years Stored unopened at 60–80°F (16–27°C)

After-Processing / Final-State Properties

Property Value Method / Condition
Cure Schedule 24–48 hours 65°F (18°C) or higher
Service Temperature -30°F to +250°F (-34°C to +121°C) Typical operating range
Tensile Strength at Break 3350 psi (23.1 MPa) ASTM D638
Elongation 9.9% ASTM D638
Young's Modulus 283,694 psi (1956 MPa) ASTM D638
Glass Transition Temperature (Tg) 141°F (61°C) ASTM E1640-99 by DMA
Cured Appearance Translucent Blue Typical

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers