LOCTITE UK3184

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

LOCTITE UK3184

Main features

  • UK 3173 System Hardener
  • 45-Minute System Work Time
  • 24-Hour Room-Temperature Cure

Product Description

LOCTITE UK 3184 Polyurethane Hardener functions as the polyurethane hardener component specified for the LOCTITE UK 3173 / UK 3184 potting system. The opaque white material has a typical viscosity of 14,000 mPa s and specific gravity of 1.45 to 1.46 at 25 deg C. When combined with UK 3173 resin at 1:4.8 by volume or 15:85 by weight, the mixture has 2,250 mPa s viscosity, a 45 minute work time, and a 24 hour room-temperature cure. Cured properties, including Shore A 80 hardness and a -15 deg C glass transition temperature, apply only to the complete resin-hardener system.

Key features

  • Dedicated UK 3173 Hardener: Specified as the hardener component for the UK 3173 / UK 3184 potting system.
  • Controlled 1:4.8 Volume Mixing: Combines with UK 3173 resin at the documented volume or weight ratio.
  • 45-Minute Potting Work Time: The complete mixed system provides a 45 minute work time at 25 deg C.

Applications

Applications include potting and encapsulation using the complete LOCTITE UK 3173 / UK 3184 resin-hardener system.

Product Family

LOCTITE UK3184

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
Viscosity
2,250 mPa.s
Viscosity (Part A)
75 mPa.s
Viscosity (Part B)
14,000 mPa.s
General Properties
Appearance
Opaque tan
Chemistry Type
Polyurethane
Mix Ratio
15 to 85
Specific Gravity
1.40
Work life @25°C
0.75 hours
Thermal Properties
Glass Transition Temperature (Tg)
-15 °C
Electrical Properties
Dielectric Strength
14,57 kV/mm
Volume Resistivity
6.61×10^12 Ohms⋅cm

Additional Information

Technical properties

Hardener properties

Values apply to the LOCTITE UK 3184 hardener component before mixing.

Property Value Unit Method / condition
Chemical type Polyurethane hardener UK 3184 component
Appearance Opaque white As supplied
Viscosity 14,000 mPa s 25 deg C, Brookfield, spindle 5, 20 rpm
Specific gravity 1.45 to 1.46 25 deg C
Technical properties

UK 3173 / UK 3184 system properties

Final-state values apply only to the complete UK 3173 / UK 3184 system, not to the hardener alone.

Property Value Unit Method / condition
Mix ratio 1:4.8 by volume UK 3173 resin : UK 3184 hardener
Mix ratio 15:85 by weight UK 3173 resin : UK 3184 hardener
Mixed viscosity 2,250 mPa s 25 deg C
Work time 45 min 300 g mass at 25 deg C
Gel time 150 min 300 g mass at 25 deg C
Cure schedule 24 h 25 deg C
Hardness 80 Shore A Cured system
Glass transition temperature -15 deg C ASTM E1545, cured system