LOCTITE UK3173

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

LOCTITE UK3173

Main features

  • Low-Viscosity Resin Handling
  • 45-Minute System Work Time
  • Flame-Retardant Potting System

Product Description

LOCTITE UK 3173 Polyurethane Potting Resin is the low-viscosity polyurethane resin component of the LOCTITE UK 3173 / UK 3184 potting system. The clear to dark-brown resin has a typical viscosity of 75 mPa s at 25 deg C and is mixed with UK 3184 hardener at 1:4.8 by volume or 15:85 by weight. The combined material has a mixed viscosity of 2,250 mPa s, a 45 minute work time, and a 24 hour room-temperature cure. The resulting flame-retardant potting compound is used for encapsulation where controlled flow, electrical insulation, and a Shore A 80 cured material are required.

Key features

  • Low-Viscosity Resin Component: The UK 3173 resin has a typical viscosity of 75 mPa s at 25 deg C.
  • Defined UK 3184 Mix Ratio: Uses 1:4.8 by volume or 15:85 by weight with the specified hardener.
  • Room-Temperature Potting Cure: The complete system cures in 24 hours at 25 deg C.

Applications

Applications include potting and encapsulation using the complete LOCTITE UK 3173 / UK 3184 resin-hardener system.

Product Family

LOCTITE UK3173

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
Viscosity
2,250 mPa.s
Viscosity (Part A)
75 mPa.s
Viscosity (Part B)
14,000 mPa.s
General Properties
Appearance
Opaque tan
Chemistry Type
Polyurethane
Mix Ratio
15 to 85
Specific Gravity
1.40
Work life @25°C
0.75 hours
Thermal Properties
Glass Transition Temperature (Tg)
-15 °C
Electrical Properties
Dielectric Strength
14,57 kV/mm
Volume Resistivity
6.61×10^12 Ohms⋅cm

Additional Information

Technical properties

Resin properties

Values apply to the LOCTITE UK 3173 resin component before mixing.

Property Value Unit Method / condition
Chemical type Polyurethane resin UK 3173 component
Appearance Clear to dark brown As supplied
Viscosity 75 mPa s 25 deg C, Brookfield, spindle 1, 20 rpm
Specific gravity 1.23 to 1.24 25 deg C
Technical properties

UK 3173 / UK 3184 system properties

Final-state values apply only when UK 3173 resin is mixed with UK 3184 hardener at the specified ratio.

Property Value Unit Method / condition
Mix ratio 1:4.8 by volume UK 3173 resin : UK 3184 hardener
Mix ratio 15:85 by weight UK 3173 resin : UK 3184 hardener
Mixed viscosity 2,250 mPa s 25 deg C
Work time 45 min 300 g mass at 25 deg C
Gel time 150 min 300 g mass at 25 deg C
Cure schedule 24 h 25 deg C
Hardness 80 Shore A Cured system
Glass transition temperature -15 deg C ASTM E1545, cured system

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers