LOCTITE UK2073

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

LOCTITE UK2073 LOCTITE UK2073

Main features

  • Low-Energy Plastic Bonding
  • Nominal 2:1 Meter-Mix Processing
  • Elastic 300% Elongation

Product Description

LOCTITE UK 2073 / LOCTITE UK 2173 Polyurethane Adhesive/Sealant System pairs two solvent-free polyurethane components for elastic bonding and sealing of plastic and multi-material automotive assemblies. Components A and B are nominally meter mixed at 2:1 by volume through a static mixer, with a 3 to 4 minute open time at 40 deg C. The room-temperature cure develops a flexible bond with 300% elongation, 3.5 to 4.5 MPa tensile strength, and Shore A 60 to 70 hardness. It is particularly suited to low-surface-energy plastics including PP talc and PP LGF, as well as PC/ABS and PC/PET, in spoilers, tailgates, roof systems, bumpers, dashboards, and trim.

Key features

  • Low-Energy Plastic Bonding: Supports PP talc, PP LGF, PC/ABS, PC/PET, and multi-material assemblies.
  • Nominal 2:1 Meter-Mix Application: The published 2:1 volume ratio is applied through a static mixer; application-specific conditions should be confirmed.
  • Elastic Cured Bond: The cured system provides 300% elongation and Shore A 60 to 70 hardness.

Applications

Applications include spoilers, tailgates, roof systems, bumpers, luggage racks, dashboards, trim, and other automotive plastic or multi-material assemblies.

Technical Specifications

Physical Properties
Open time
3 to 4 minutes
Viscosity (Part B)
30,000 to 100,000 mPa.s
General Properties
Mix Ratio
2 :1
Mechanical Properties
Elongation
300 %

Additional Information

Technical properties

Component properties

Component A and Component B values are listed separately before 2:1 volume mixing.

Property Value Unit Method / condition
Component A appearance Black As supplied
Component A density 1.35 g/cm^3 23 deg C
Component A viscosity 60 to 100 Pa s 23 deg C, rheometer
Component B appearance Gray As supplied
Component B density 1.38 g/cm^3 23 deg C
Component B viscosity 30 to 100 Pa s 23 deg C, rheometer
Mix ratio 2:1 by volume Component A : Component B; published nominal ratio
Technical properties

Mixed and cured system properties

Values apply to the complete LOCTITE UK 2073 / LOCTITE UK 2173 system.

Property Value Unit Method / condition
Open time 3 to 4 min 40 deg C
Tensile shear strength >2.5 MPa After 3 days at 23 deg C on documented plastic and e-coated steel substrates
Elongation at break 300 % Cured system
Tensile strength 3.5 to 4.5 MPa Cured system
Hardness 60 to 70 Shore A Cured system
Final strength development 3 days Room-temperature cure