LOCTITE TC8M

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

LOCTITE TC8M

Main features

  • High Thermal-Conductivity Silicone Grease
  • Electrical-Insulation Thermal Grease
  • Corrosion-Protective Thermal Grease

Product Description

LOCTITE® TC 8M is a silicone-based thermal grease formulated for efficient heat transfer between heat-generating electronic components and heat-dissipating structures. The material combines high thermal conductivity with excellent electrical insulation and dielectric properties, making it suitable for a broad range of thermal management applications. It retains its paste-like consistency during prolonged exposure to elevated temperatures and is designed for use in semiconductor devices, thermoelectric equipment, radiators, power resistors, and chassis-mounted components. Based on the uploaded datasheet image.

Key Features & Benefits

  • High thermal conductivity for efficient heat dissipation.
  • Excellent electrical insulation properties.
  • High dielectric strength.
  • Maintains paste consistency at elevated temperatures.
  • Suitable for thermal interface applications.
  • Provides corrosion protection on mating surfaces.
  • Easy application using syringes, cartridges, and dispensing equipment.

Recommended Applications

  • Heat sinks in semiconductor devices.
  • Thermostats in thermoelectric devices.
  • Radiators and mounting surfaces.
  • Power resistors.
  • Electronic chassis assemblies.
Product Family

LOCTITE TC8M

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
white
Density (g)
2.5 g/cm3
Physical Properties
Viscosity
1300 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Silicone Grease — Thermal management compound
Appearance White — As supplied
Viscosity 1,300 mPa·s (cP) 25°C, 0.5 rpm
Viscosity 330 mPa·s (cP) 25°C, 5 rpm
Density 2.5 g/cm³ Typical value
Fineness <50 µm Typical value
Shelf Life 365 days 18 to 25°C storage
Operating Temperature Range -40 to +200 °C Continuous operation
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Thermal Conductivity 1.5 W/(m·K) Physical property
Weight Loss 0.2 % 24 h @ 100°C
Dielectric Strength 19 kV/mm Electrical property
Volume Resistivity 1 × 10¹⁴ Ω·cm Electrical property
Thermal Management Performance High — Enhances heat transfer between components
Electrical Insulation High — High dielectric and resistivity properties
High Temperature Stability Excellent — Retains paste consistency after heat exposure