LOCTITE TC4

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

LOCTITE TC4

Main features

  • Thermally Conductive Lubrication
  • High Insulation Resistance
  • High Dielectric Strength

Product Description

LOCTITE® TC 4 is a silicone-based thermal grease designed to provide efficient heat transfer between heat-generating electronic components and heat-dissipating structures. The material offers high thermal conductivity, high insulation resistance, and high dielectric strength while maintaining a stable paste-like consistency even after prolonged exposure to elevated temperatures. It is widely used in thermal management applications involving semiconductors, power electronics, thermostats, and heat sinks.

Key Features & Benefits

  • High thermal conductivity for efficient heat transfer.
  • High insulation resistance.
  • High dielectric strength.
  • Maintains paste consistency during long-term high-temperature exposure.
  • Provides corrosion protection on mating surfaces.
  • Suitable for electronic thermal management systems.
  • Easy application by brush, syringe, cartridge, or dispensing equipment.

Recommended Applications

  • Heat sinks in semiconductor devices.
  • Thermoelectric devices and radiators.
  • Thermostat mounting surfaces.
  • Power resistors mounted on chassis.
  • General electronic heat-transfer interfaces.
Product Family

LOCTITE TC4

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
White
Specific Gravity
2.35
Thermal Properties
Thermal Conductivity
0.6 W/m.K
Electrical Properties
Dielectric Strength
19.7 kV/mm

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Silicone Grease — Thermal management compound
Appearance White — As supplied
Density 2.35 g/cm³ Typical value
Shelf Life 365 days 18 to 25°C storage
Operating Temperature Range -40 to +200 °C Continuous service
Application Type Thermal Management — Heat transfer interface material
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Thermal Conductivity 0.6 W/(m·K) Typical cured property
Hardness 20 - 25 Shore A Physical property
Dielectric Strength 19.7 kV/mm Electrical property
Volume Resistivity 1 × 10¹³ Ω·cm Electrical property
High Temperature Stability Excellent — Will not harden after prolonged heat exposure
Heat Transfer Efficiency High — Electronic thermal interface applications
Electrical Insulation High — High insulation resistance and dielectric strength

Leading Brands Trust in Our Products and Services