LOCTITE® SICOMET 100 is a fast-curing, medium-viscosity ethyl cyanoacrylate instant adhesive designed for bonding a wide range of materials including plastics, rubbers, metals, fabrics, and foam materials. The one-component adhesive cures rapidly through surface moisture and develops handling strength within seconds on close-fitting parts. It offers excellent adhesion to plastics and elastomers while requiring no mixing, making it suitable for high-speed assembly and repair operations.

Key Features & Benefits

  • Ethyl cyanoacrylate instant adhesive technology.
  • Excellent adhesion to rubbers and plastics.
  • Fast fixture and cure speed.
  • Medium-low viscosity for easy application.
  • One-component formulation requiring no mixing.
  • Easy dispensing and handling.
  • Suitable for close-fitting assemblies.

Recommended Applications

  • Plastic component assembly.
  • Rubber and elastomer bonding.
  • Foam material bonding.
  • Metal bonding applications.
  • Fabric assembly and repair.
  • General-purpose instant bonding operations.
Product Family

LOCTITE SICOMET 100

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Colorless liquid
Specific Gravity
1.05 - 1.10
Physical Properties
Viscosity
140 - 220 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Ethyl Cyanoacrylate — Instant adhesive
Appearance Colourless Liquid — Uncured material
Components One Part — No mixing required
Viscosity Classification Medium-Low — Product characteristic
Specific Gravity 1.05 - 1.10 — 25°C
Viscosity 140 - 220 mPa·s (cP) 25°C
Cure Mechanism Surface Moisture — Moisture activated
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Recommended Gap Fill 0.01 - 0.50 mm Typical bond gap
Fixture Time (Aluminium) 5 - 10 seconds Typical cure speed
Fixture Time (Steel) 10 - 30 seconds Typical cure speed
Fixture Time (Rubber, Nitrile) 5 - 10 seconds Typical cure speed
Fixture Time (ABS) 5 - 10 seconds Typical cure speed
Fixture Time (PVC) 5 - 10 seconds Typical cure speed
Tensile Shear Strength (Steel) 17 N/mm² ISO 4587, 24 h cure
Tensile Shear Strength (Aluminum) 15 N/mm² ISO 4587, 24 h cure
Tensile Shear Strength (ABS) 8* N/mm² Substrate failure