LOCTITE SI 5293

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE SI 5293

Main features

  • PCB/Electronics Protection
  • UV and moisture cure
  • Alkoxy Silicone

Product Description

Loctite SI 5293 is a conformal coating designed to provide environmental protection for printed circuit boards and other sensitive electronic components. It is an alkoxy silicone that is fluorescent under UV light, and exposed to sufficient UV light irradiance to cure the material effectively. 

Loctite SI 5293  is a one-component material that doesn't require mixing. It is an encapsulant that can cure primary by UV exposure and secondary by moisture in shadowed areas. 

 

Advantages of Loctite SI 5293

  • PCB/Electronic component environmental protection
  • One component - No mixing required
  • Transparent amber to yellow liquid
  • Excess material can be easily removed with non-polar solvents
  • Functional strength is achieved almost instantly

 

Cure Schedule

  • 60 seconds @ 70mW/cm^2 (per side)

Although functional strength is developed almost instantly due to the UV-curing nature of LOCTITE SI 5293, increased cure properties are developed during 72 hours at ambient conditions. 

Product Family

LOCTITE SI 5293

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific Gravity
1
Thermal Properties
Glass Transition Temperature (Tg)
-40 °C
Thermal Conductivity
0.18 W/m.K
Electrical Properties
Volume Resistivity
100000000000000 Ohms⋅cm
Mechanical Properties
Elongation
15 %