Product Description

LOCTITE® SI 5210™ is an ultra-fast curing, non-corrosive RTV alkoxy silicone formulated for potting, wire tacking, selective sealing, vibration damping, and repair or rework applications on printed circuit boards and electronic assemblies. The thixotropic, non-sag formulation minimizes migration after application while providing rapid surface cure for high-volume manufacturing environments. It delivers excellent environmental resistance, flexibility, and electrical insulation performance for demanding industrial and electronics applications. Based on the uploaded datasheet image.

Key Features & Benefits

  • Ultra-fast curing RTV silicone formulation.
  • Non-corrosive alkoxy cure system.
  • Thixotropic paste minimizes material migration.
  • Suitable for potting, sealing and wire tacking.
  • Excellent vibration damping properties.
  • Rapid handling strength after dispensing.
  • Designed for high-volume electronics manufacturing.
  • Excellent environmental resistance.

Recommended Applications

  • PCB potting and protection.
  • Wire tacking applications.
  • Selective electronic sealing.
  • Vibration damping assemblies.
  • Repair and rework operations.
  • Automotive electronics protection.
Product Family

LOCTITE SI 5210

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Translucent to opaque, slightly yellow to straw color paste
Specific Gravity
1.05

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Silicone — RTV potting compound
Chemical Type Alkoxy Silicone — Non-corrosive cure system
Appearance Translucent to Opaque, Slightly Yellow to Straw Paste — Uncured material
Components One Component — No mixing required
Viscosity Thixotropic Paste — Non-sag formulation
Specific Gravity 1.05 — 25°C
Extrusion Rate 100 - 700 g/min 0.62 MPa, 25°C, 1/8 in nozzle
Tack-Free Time ≤5 minutes 22°C / 50% RH
Depth of Cure 2.0 mm After 4 hours
Depth of Cure 3.4 mm After 16 hours
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Shore Hardness 48 Shore A ISO 868, cured 1 week
Water Vapor Transmission Rate 5.2 g/(h·m²) Typical cured value
Water Absorption 0.87 % 24 h immersion at room temperature
Glass Transition Temperature -52 °C Typical cured value
Coefficient of Thermal Expansion 255 µm/m·K Typical cured value
Elongation at Break 230 % Typical cured value
Tensile Strength 2.8 N/mm² Typical cured value
Tear Strength 9.5 N/mm ISO 34-1
Dielectric Breakdown Strength 20.1 kV/mm IEC 60243-1
Volume Resistivity 8.2 × 10¹⁴ Ω·cm IEC 60093
Lap Shear Strength (Aluminum) 1.3 N/mm² ISO 4587, cured 1 week