LOCTITE SF7701

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE SF7701

Main features

  • Low-Energy Plastic Priming
  • Fast 30-Second Drying
  • UV-Visible Primer Inspection

Product Description

LOCTITE SF 7701 Primer is a clear, one-part n-heptane primer for preparing polyolefin and other low-energy surfaces for bonding with LOCTITE cyanoacrylate adhesives. The very-low-viscosity liquid contains 0.08% to 0.12% active ingredient, dries in 30 seconds or less at 20 deg C, and remains active on the part for up to 8 hours. It is intended for difficult-to-bond materials including polyethylene, polypropylene, PTFE, and thermoplastic rubber. The primer also accelerates cyanoacrylate fixture, while maximum bond strength develops after 24 hours at 22 deg C.

Key features

  • Low-energy surface priming: Prepares polyethylene, polypropylene, PTFE, and thermoplastic rubber for cyanoacrylate bonding.
  • Fast 30-second drying: Dries in 30 seconds or less at 20 deg C before adhesive application.
  • UV-visible primer inspection: Primer presence can be checked with a 365 nm UV inspection lamp.

Applications

Applications include priming low-energy plastics for LOCTITE cyanoacrylate bonding.

Product Family

LOCTITE SF7701

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Clear colorless liquid
Chemistry Type
Aliphatic amine
Solvent
n-heptane
Specific Gravity
0.68
Physical Properties
Drying Time
<30 seconds
Viscosity
1.25 mPa.s

Additional Information

Technical properties

As-supplied properties

Property Value Unit Method / condition
Appearance Clear colorless liquid As supplied
Active ingredient concentration 0.08 to 0.12 % Aliphatic amine
Fluorescence Positive Under UV light
Specific gravity 0.68 25 deg C
Viscosity 1.25 mPa s (cP) 20 deg C