LOCTITE SF770

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

LOCTITE SF770

Main features

  • Cyanoacrylate Adhesion Primer
  • Low-Surface-Energy Plastic Bonding
  • 8 to 9-Second Dry Time

Product Description

LOCTITE® SF 770 is a cyanoacrylate surface primer specifically formulated to improve adhesion on difficult-to-bond, low surface energy plastics such as polyethylene (PE), polypropylene (PP), polytetrafluoroethylene (PTFE), and thermoplastic rubber materials. The primer modifies the surface characteristics of these substrates, enabling LOCTITE® cyanoacrylate adhesives to achieve substantially improved bond performance. It is recommended only for low-energy plastics and can be detected under UV light after application.

Key Features & Benefits

  • Surface primer for cyanoacrylate adhesives.
  • Improves bonding to low surface energy plastics.
  • Suitable for polyethylene, polypropylene and PTFE.
  • Very low viscosity for uniform surface coverage.
  • Fluoresces under UV light for inspection.
  • Can be applied by spray, brush or dipping methods.
  • Extends cyanoacrylate bonding capability to difficult substrates.

Recommended Applications

  • Polyethylene component bonding.
  • Polypropylene assembly applications.
  • PTFE bonding preparation.
  • Thermoplastic rubber bonding.
  • General low-energy plastic surface preparation.
Product Family

LOCTITE SF770

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Transparent to slightly hazy liquid
Specific Gravity
0.87
Physical Properties
Viscosity
0.82 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Primer for Cyanoacrylate — CA surface primer
Chemical Type Aliphatic Amine — Active primer chemistry
Solvent Isopropyl Acetate — Carrier solvent
Appearance Transparent to Slightly Hazy Liquid — As supplied
Fluorescence Positive Under UV Light — Inspection aid
Specific Gravity 0.87 — 23°C
Viscosity 0.62 mPa·s (cP) Cone & Plate, 25°C
Drying Time (Steel) 9 seconds 23°C
Drying Time (Polypropylene) 9 seconds 23°C
Drying Time (Polyethylene) 8 seconds 23°C
On-Part Life 8 hours Typical
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Block Shear Strength (PP + LOCTITE® 406) 15 N/mm² ISO 13445, 24 h cure @ 23°C
Block Shear Strength (PP + LOCTITE® 496) 4.8 N/mm² ISO 13445
Block Shear Strength (PP + LOCTITE® 460) 13 N/mm² ISO 13445
Block Shear Strength (Acetal + LOCTITE® 406) 14 N/mm² ISO 13445
HDPE to Mild Steel (LOCTITE® 406) 15 N/mm² Primer on HDPE
Polypropylene to Polypropylene (LOCTITE® 406) 13 N/mm² Primer on polypropylene
Water Resistance 100% Strength Retention After 1000 h water exposure
Humidity Resistance 100% Strength Retention 95% RH, 1000 h exposure