LOCTITE SF768

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

LOCTITE SF768

Main features

  • Cyanoacrylate Residue Removal
  • Very-Low-Viscosity Solvent Cleaner
  • Surface Cleaning and Debonding

Product Description

LOCTITE® SF 768™ is a solvent-based cleaner formulated specifically for the removal of cured cyanoacrylate adhesives and for debonding components assembled with instant adhesives. The low-viscosity blend of nitromethane and hydrocarbon solvents penetrates cured adhesive deposits, allowing adhesive residues to be softened and removed from surfaces. It is suitable for maintenance, rework, and cleaning applications involving cured cyanoacrylate contamination. Based on the uploaded datasheet image.

Key Features & Benefits

  • Specialized solvent cleaner for cured cyanoacrylate removal.
  • Designed to debond cyanoacrylate-assembled parts.
  • Very low viscosity for rapid penetration.
  • Suitable for surface cleaning and adhesive residue removal.
  • Can soften cured adhesive in minutes to hours depending on thickness.
  • Effective on thin films, thick beads and assembled components.

Recommended Applications

  • Removal of cured cyanoacrylate adhesive residues.
  • Debonding assemblies bonded with instant adhesives.
  • Cleaning contaminated surfaces.
  • Maintenance and repair operations.
  • Rework of cyanoacrylate-bonded components.
Product Family

LOCTITE SF768

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Clear to yellow
Specific Gravity
1.1
Physical Properties
Viscosity
1.5 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Solvent Cleaner — Cyanoacrylate adhesive remover
Chemical Type Nitromethane / Hydrocarbon — Solvent blend
Appearance Clear to Yellow — As supplied
Viscosity Very Low — Product characteristic
Specific Gravity 1.1 — 25°C
Viscosity 1.5 mPa·s (cP) 20°C
Cure Not Applicable — Cleaner product
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Thin Adhesive Layer Removal Wipes Off Easily — Using SF 768 soaked cloth or tissue
Thick Bead Removal Time 15 to 30 minutes May require reapplication
Bonded Assembly Soak Time Several Hours — For debonding assembled parts
Adhesive Softening Rate Several Minutes to Several Hours — Depends on adhesive quantity
Cyanoacrylate Debonding Effective — For cured CA adhesive assemblies
Cleaning Function Surface Residue Removal — Maintenance and rework operations
Reapplication Requirement May Be Required — For thick adhesive deposits