LOCTITE SF7649

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE SF7649

Main features

  • Thirty-Day On-Part Life
  • Low-Temperature Cure Acceleration
  • Brush, Spray, or Pre-Applied Use

Product Description

LOCTITE SF 7649 Primer N Activator is a one-part acetone-based surface treatment that accelerates cure of LOCTITE anaerobic adhesives and sealants. The transparent green liquid can be brushed, sprayed, or pre-applied and dries in 30 to 70 seconds at 20 deg C. It is used on passive metals, inactive surfaces, large bond gaps, and assemblies below 15 deg C. Activated parts can remain ready for bonding for up to 30 days when protected from contamination. After the solvent evaporates, the anaerobic adhesive is applied separately and the assembly is secured until fixtured.

Key features

  • Thirty-day activation window: Activated surfaces remain ready for bonding for up to 30 days when kept clean.
  • Low-temperature cure acceleration: Promotes anaerobic cure on passive or inactive surfaces below 15 deg C.
  • Multiple application methods: Supports brush, spray, and pre-applied surface treatment.

Applications

Applications include anaerobic priming, gasketing, pipe sealing, retaining, thread sealing, and threadlocking where increased cure speed is required.

Product Family

LOCTITE SF7649

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Transparent, green liquid
Chemistry Type
Copper salt and aliphatic amine
Solvent
Acetone
Specific Gravity
0.79
Physical Properties
Drying Time
30-70 seconds
Viscosity
2 mPa.s

Additional Information

Technical properties

As-supplied properties

Property Value Unit Method / condition
Appearance Transparent green liquid As supplied
Specific gravity 0.79 25 deg C
Viscosity 2 mPa s (cP) 20 deg C

Leading Brands Trust in Our Products and Services