LOCTITE SF7471

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE SF7471

Main features

  • Fast 30-70 Second Drying
  • Low-Temperature Cure Acceleration
  • Seven-Day On-Part Life

Product Description

LOCTITE SF 7471 Activator is a one-part acetone/isopropanol solvent activator for increasing the cure speed of LOCTITE anaerobic adhesives and sealants. The transparent yellow-to-amber liquid is applied by spray or brush and dries in 30 to 70 seconds at 20 deg C. It is used on passive metals, inert surfaces, large bond gaps, and assemblies below 15 deg C where anaerobic cure is slower. Treated surfaces remain active for up to 7 days when protected from contamination. The activator and adhesive are applied separately and must not be mixed together as liquids.

Key features

  • Fast surface activation: Dries in 30 to 70 seconds at 20 deg C before adhesive assembly.
  • Low-temperature cure assistance: Accelerates anaerobic cure in applications below 15 deg C.
  • Seven-day on-part life: Activated surfaces remain usable for up to 7 days when kept clean.

Applications

Applications include cure acceleration for LOCTITE anaerobic adhesives and sealants on passive metals or inert surfaces, in large-gap assemblies, and below 15 deg C.

Product Family

LOCTITE SF7471

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Transparent, yellow to amber liquid
Chemistry Type
Amine and Thiazole
Specific Gravity
0.79
Physical Properties
Drying Time
30-70 seconds
Viscosity
2 mPa.s

Additional Information

Technical properties

As-supplied properties

Property Value Unit Method / condition
Appearance Transparent yellow to amber liquid As supplied
Specific gravity 0.79 25 deg C
Viscosity 2 mPa s (cP) 20 deg C

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers