LOCTITE SF 7387
Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other
Main features
- Activator
- Very low viscosity
- Promote cure of acrylic adhesives
Product Description
LOCTITE® SF 7387 is a yellow to amber, transparent liquid substituted dihydropyridine activator containing the solvents n-Heptane and isopropanol.
LOCTITE® SF 7387 is designed for LOCTITE toughened adhesives to initiate the cure of acrylic adhesives.
Packaging
Please select Package Type.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Specific Gravity
0.8
Physical Properties
Viscosity
1 mPa.s