LOCTITE SF7090

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

LOCTITE SF7090

Main features

  • Accelerates Cure of Loctite Anaerobic Adhesives
  • Solvent-Free Bonding Formulation
  • Passive Metals and Inert Materials

Product Description

LOCTITE® SF 7090™ is a reactive monomer-based, solvent-free surface activator designed to accelerate the cure speed of LOCTITE® anaerobic adhesives and sealants. It is particularly effective for use on passive metals, inert surfaces, large bond gaps, and low-temperature applications below 15°C. The activator promotes rapid fixture and cure development while remaining active on treated surfaces for up to one hour after application.

Key Features & Benefits

  • Accelerates cure of LOCTITE® anaerobic adhesives and sealants.
  • Solvent-free reactive monomer formulation.
  • Ideal for passive metals and inert substrates.
  • Improves curing across large bond gaps.
  • Recommended for low-temperature applications (<15°C).
  • Can be applied by spray or brush.
  • Remains active on surfaces for up to one hour.

Recommended Applications

  • Acceleration of anaerobic threadlockers.
  • Acceleration of anaerobic retaining compounds.
  • Passive metal assemblies.
  • Large bond gap assemblies.
  • Low-temperature bonding operations.
Product Family

LOCTITE SF7090

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Dark blue-green liquid
Specific Gravity
1.03
Physical Properties
Viscosity
10 - 25 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Activator — For anaerobic adhesives and sealants
Chemical Type Copper Salt and Aliphatic Amine — Reactive activator chemistry
Solvent Reactive Methacrylate Monomer — Solvent-free system
Appearance Dark Blue-Green Liquid — As supplied
Specific Gravity 1.03 — 25°C
Viscosity 10 - 25 mPa·s (cP) Brookfield RVT, 25°C
Part Life ≤1 hour Activated surface life
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Fixture Time ≤25 seconds Steel, ISO 4587, LOCTITE® 326™, two-side activation
Activator Open Time Up to 1 hour Activator remains effective after application
Application Method Spray or Brush — Apply to mating surfaces
Large Gap Performance Enhanced — Promotes cure in larger bond gaps
Passive Metal Performance Enhanced — Improves cure on passive substrates
Low Temperature Suitability Recommended — Below 15°C operating conditions
Cure Acceleration Function High — For LOCTITE anaerobic products

Leading Brands Trust in Our Products and Services