LOCTITE SF7070

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE SF7070

Main features

  • Low-Viscosity Precision Cleaning
  • 5-20 Minute Drying Window
  • Spray, Wipe, or Immersion Use

Product Description

LOCTITE SF 7070 Cleaner and Degreaser is a one-part, non-aqueous hydrocarbon and monoterpene solvent cleaner for final pre-assembly surface preparation. The colorless, very-low-viscosity liquid removes greases, oils, lubricating fluids, metal cuttings, and fines before bonding with LOCTITE adhesives. It can be applied by spray, wipe, or immersion at room temperature or with controlled heating. The cleaner typically dries in 5 to 20 minutes at 20 deg C and does not change adhesive cure speed or final strength beyond providing a clean bonding surface.

Key features

  • Low-viscosity surface cleaning: A 1 to 2 mPa s liquid reaches detailed surfaces for spray, wipe, or immersion cleaning.
  • Pre-bond contaminant removal: Removes oils, greases, lubricating fluids, metal cuttings, and fines before adhesive assembly.
  • Controlled drying window: Typically evaporates in 5 to 20 minutes at 20 deg C before bonding.

Applications

Applications include final pre-assembly cleaning and degreasing by spray, wipe, or immersion before bonding.

Product Family

LOCTITE SF7070

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Colorless transparent liquid
Chemistry Type
Hydrocarbon / Monoterpene blend
Specific Gravity
0.75
Physical Properties
Drying Time
5-20 minutes
Viscosity
1-2 mPa.s

Additional Information

Technical properties

As-supplied properties

Property Value Unit Method / condition
Appearance Colorless transparent liquid As supplied
Specific gravity 0.75 25 deg C
Viscosity 1 to 2 mPa s (cP) 20 deg C
Kauri-butanol value 31 Typical property