Main features

  • Rapid 90-Minute Full Cure
  • Self-Leveling Low-Viscosity Fill
  • 10-15% Joint Movement Capability

Product Description

LOCTITE PC 6231 Rapid-Curing Concrete Joint Filler is a two-part, 1:1 mixed, self-leveling material for filling and repairing interior control joints and new saw-cut joints in horizontal concrete. The 100% solids, low-viscosity system gels in 3 minutes and cures in 90 minutes at 24 deg C, allowing traffic after full cure. It accommodates 10% to 15% movement of installed joint width. The cured material combines 1.9 N/mm^2 adhesion to concrete, 82% elongation, and Shore A 75 to 80 hardness for heavy-traffic and freezer-floor applications.

Key features

  • Rapid 90-minute cure: Gels in 3 minutes and reaches full cure in 90 minutes at 24 deg C.
  • Self-leveling joint fill: A mixed viscosity of 525 mPa s supports gravity feeding into prepared horizontal joints.
  • Controlled joint movement: Accommodates 10% to 15% movement of installed joint width.

Applications

Applications include interior control joints, new-construction saw-cut joints, heavy-traffic industrial floors, freezer floors, and exterior horizontal concrete with minimal thermal movement.

Technical Specifications

General Properties
Appearance
Gray
Chemistry Type
Polyurethane
Component System
2K
Mix Ratio
1 : 1
Physical Properties
Viscosity
525 mPa.s
Viscosity (Part B)
392 to 1,142 mPa.s
VOC
1.7 g/l
Mechanical Properties
Elongation
82 %

Additional Information

Technical properties

As-supplied properties

Component values are reported separately; mixed properties apply after 1:1 volume mixing.

Property Value Unit Method / condition
Mix ratio 1:1 By volume, resin:hardener
Resin viscosity 586 to 1,186 mPa s (cP) 25 deg C
Hardener viscosity 392 to 1,142 mPa s (cP) 25 deg C
Mixed viscosity 525 mPa s (cP) 25 deg C
Resin weight per gallon 8.89 to 9.29 lb/gal As supplied
Hardener weight per gallon 8.47 to 8.87 lb/gal As supplied
Mixed VOC 1.7 g/L Mixed material
Technical properties

Cured and installed properties

Cured-material values apply after 7 days at 25 deg C unless another condition is shown.

Property Value Unit Method / condition
Adhesion to concrete 1.9 N/mm^2 ASTM D4541; cured 7 days at 25 deg C
Tensile strength 8.3 N/mm^2 ASTM D412 / ISO 37; 24 deg C; cured 7 days at 25 deg C
Elongation 82 % ASTM D412 / ISO 37; cured 7 days at 25 deg C
Shore hardness 75 to 80 Shore A ISO 868; cured 7 days at 25 deg C
Joint movement capability 10 to 15 % Installed joint width