LOCTITE MR5412

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

LOCTITE MR5412

Main features

  • Solvent-Based Neoprene Contact Adhesive
  • Fast Air-Dry Tack
  • Repositionable During Initial Assembly

Product Description

LOCTITE® MR 5412 is a solvent-based neoprene rubber contact adhesive designed for maintenance, repair, and general-purpose bonding applications. The adhesive develops fast, high-strength bonds and provides waterproof performance on both porous and non-porous substrates. It is particularly suitable for bonding weatherstripping, insulation, rubber components, and trim materials to wood and metal surfaces, while allowing repositioning during assembly before final bond formation.

Key Features & Benefits

  • Solvent-based neoprene rubber contact adhesive.
  • Fast, high-strength bond development.
  • Waterproof bond performance.
  • Repositionable during initial assembly.
  • Suitable for porous and non-porous substrates.
  • Air-dry curing system.
  • Strength increases with aging and moderate heat exposure.

Recommended Applications

  • Weatherstripping installation and repair.
  • Insulation bonding.
  • Rubber-to-metal bonding.
  • Trim attachment applications.
  • Wood-to-rubber and wood-to-metal bonding.
  • General maintenance and repair bonding.
Product Family

LOCTITE MR5412

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Yellow liquid
Specific Gravity
0.88
Physical Properties
Viscosity
6,000 - 10,000 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Solvent Based Contact Adhesive — Neoprene rubber formulation
Chemical Type Neoprene Rubber — Contact cement chemistry
Appearance Yellow Liquid — As supplied
Specific Gravity 0.88 — 25°C
Viscosity 6,000 - 10,000 mPa·s (cP) Brookfield RV, 25°C
Solids Content 30 - 34 % Non-volatile content
Weight per Gallon 7.01 - 8.56 lb/gal Typical
Cure Mechanism Air Dry — Solvent evaporation
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Benefit
Open Time Before Assembly 3 - 4 minutes Allow adhesive to become tacky
Initial Bond Strength High — Holds most assemblies immediately
Final Bond Strength Maximum After Full Drying — Strength develops as solvent evaporates
Water Resistance Waterproof — Suitable for weatherstrip applications
Repositionability Yes — Allows adjustment during assembly
Porous Surface Compatibility Suitable — Wood, insulation and similar materials
Non-Porous Surface Compatibility Suitable — Metal and rubber bonding
Heat Aging Performance Improved Strength — Moderate heat exposure increases bond strength