LOCTITE M4100 E&C

Harmonization Code : 32159090 | Printing ink, writing or drawing ink, and other inks, whether or not concentrated or solid, specifically for those classified as other within that category

LOCTITE M4100 E&C

Main features

  • Conductive
  • screen printable
  • Electroless nickel plateable

Product Description

LOCTITE M 4100 MINICO E&C electroless nickel plateable conductive polymer is designed as a terminator where the M2000 RS MINICO E&C polymer resistor series has been applied.

LOCTITE M 4100 MINICO E&C is designed to be applied using standard screen printing methods.

Product Family

LOCTITE M4100

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 131 days
CA Shipping in 8 weeks
EU Shipping in 60 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g)
2800000 g/cm3
Solids
78 %
Physical Properties
Viscosity
45 mPa.s

Additional Information

Storage
Store product in the unopened container in a dry location. Storage information may be indicated on the product container labeling.

Store in a cool, well ventilated area.

Optimal Storage : 18 to 25 °C


Material removed from containers may be contaminated during use. Do not return product to the original container. Henkel Corporation cannot assume responsibility for product which has been contaminated or stored under conditions other than those previously indicated. 