Main features

  • Visible 10:1 Mix Confirmation
  • 30-Minute Assembly Window
  • Resilient Peel and Impact Performance

Product Description

LOCTITE AA H8000 is a two-component, non-sag methacrylate structural adhesive for metals, plastics and composites. Yellow resin and blue hardener mix at 10:1 by volume to create a green adhesive that visibly indicates mixed material. At 25 deg C, the mixed adhesive has a typical cone-and-plate viscosity of 8,850 mPa s and a 30 minute working time on steel, aluminum and polyethylene. Fixture time on grit-blasted mild steel is typically 25 to 30 minutes. The cured adhesive combines resilient bonding with peel, impact and lap-shear performance across specified substrates.

Key features

  • Visible green mix: Yellow resin and blue hardener produce a green mixed adhesive for process confirmation.
  • 30-minute working time: The mixed system provides a 30 minute assembly window at 25 deg C on the stated substrates.
  • Non-sag structural bonding: The methacrylate system supports controlled application on metals, plastics and composites.

Applications

Applications include structural bonding of metals, plastics and composites, including steel, aluminum, stainless steel, FRP, gelcoat and ABS.

Product Family

LOCTITE H8000

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
Viscosity
8,850 mPa.s
Viscosity (Part A)
6,700 mPa.s
Viscosity (Part B)
6,530 mPa.s
General Properties
Appearance
Green
Chemistry Type
Methacrylate
Mix Ratio
10 : 1
Specific Gravity
0.98
Work life @25°C
0.5 hours
Mechanical Properties
Elongation
13 %
Peel Strength
8
Thermal Properties
Glass Transition Temperature (Tg)
71 °C
Curing Conditions
Fixture Time
25 to 30 minutes

Additional Information

Technical properties

As-supplied properties

Part A, Part B and mixed-system values before cure.

Property Value Unit Method / condition
Part A appearanceYellowResin component
Part B appearanceBlueHardener component
Mixed appearanceGreenAfter 10:1 volume mixing
Mix ratio by volume10:1Part A to Part B
Part A viscosity6,700mPa sCone CP50-1, shear rate 50 s^-1, 25 deg C
Part B viscosity6,530mPa sCone CP50-1, shear rate 50 s^-1, 25 deg C
Mixed viscosity8,850mPa sCone CP50-1, shear rate 50 s^-1, 25 deg C
Working time30minutesAt 25 deg C on steel, aluminum and polyethylene
Technical properties

Final-state properties

Physical properties and cured adhesive performance; cure conditions are listed per row where stated.

Property Value Unit Method / condition
Glass transition temperature71deg CISO 11359-2
Shore hardness70Shore DISO 868
Elongation at break13%ISO 527-2
Tensile strength at break15N/mm^2ISO 527-2
Tensile modulus1,080N/mm^2ISO 527-2
Impact strength23JISO 9653, grit-blasted mild steel, cured 72 hours at 22 deg C
T-peel strength8N/mmISO 11339, steel, cured 72 hours at 22 deg C
Lap shear strength24N/mm^2Grit-blasted mild steel, cured 72 hours at 22 deg C