LOCTITE H4500

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

LOCTITE H4500

Main features

  • 15-Minute Working Time
  • High Impact and Peel Strength
  • Primerless Structural Bonding

Product Description

LOCTITE® AA H4500™ is a two-component methacrylate structural adhesive designed to provide resilient, high-strength bonds across a wide variety of substrates including metals, plastics, composites, and coated surfaces. The adhesive cures at room temperature, offers excellent environmental durability, superior impact and peel strength, and tolerates off-ratio mixing. Its thixotropic, non-sag formulation can fill gaps up to 12.7 mm and does not require a primer for most applications.

Key Features & Benefits

  • Two-component methacrylate structural adhesive.
  • Excellent environmental resistance.
  • Superior impact and peel strength.
  • Excellent tolerance to off-ratio mixing.
  • Primerless bonding on many substrates.
  • Non-sag formulation fills gaps up to 12.7 mm.
  • Non-corrosive cured adhesive system.

Recommended Applications

  • Steel and stainless steel bonding.
  • Aluminum assembly applications.
  • Epoxy-coated metal structures.
  • Sheet molding compound (SMC) assemblies.
  • Engineering plastic and composite bonding.
Product Family

LOCTITE H4500

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Gray
Specific Gravity
0.99/0.96
Physical Properties
Viscosity
14,900/9,200 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Methacrylate Adhesive — Two-component acrylic system
Appearance (Part A) White — Resin
Appearance (Part B) Black Viscous Liquid — Hardener
Appearance (Mixed) Gray — Mixed adhesive
Mix Ratio 10 : 1 Part A : Part B By volume
Specific Gravity (Part A) 0.99 — 25°C
Specific Gravity (Part B) 0.96 — 25°C
Viscosity (Part A) 14,900 mPa·s (cP) 25°C
Viscosity (Part B) 9,200 mPa·s (cP) 25°C
Working Time 15 minutes 25°C
Fixture Time 10 - 15 minutes ISO 4587, steel
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Glass Transition Temperature (Tg) 107 °C ISO 11359-2
Shore Hardness 73 Shore D ISO 868
Elongation at Break 11 % ISO 527-2
Tensile Strength at Break 19.5 N/mm² ISO 527-2
Tensile Strength at Yield 32 N/mm² ISO 527-2
Tensile Modulus 1,370 N/mm² ISO 527-2
Lap Shear Strength (Stainless Steel) ≥20.7 N/mm² 24 h @ 22°C
Lap Shear Strength (Aluminum) 21 N/mm² 72 h @ 22°C
Impact Strength (Steel) 12 J ISO 9653
T-Peel Strength (Steel) 10 N/mm ISO 11339

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers