LOCTITE EF562S LOCTITE EF562S

Main features

  • Non-Asbestos Honeycomb Bonding
  • Roll-or-Sheet Layup Flexibility
  • Expanding Core Reinforcement

Product Description

LOCTITE EF 562S AERO is a non-asbestos, unsupported modified epoxy foaming film adhesive for sealing, splicing and reinforcing honeycomb materials. Supplied in roll or sheet form, the film is cut and positioned during lay-up before heat cure. Its expanding behavior fills localized honeycomb details, while the unsupported construction allows direct placement without a carrier fabric. The product supports aerospace honeycomb fabrication processes that specify EF 562S and its specified cure and expansion conditions.

Key features

  • Non-asbestos formulation: The modified epoxy foaming adhesive is supplied without asbestos reinforcement.
  • Roll or sheet format: The unsupported film is available in forms suited to cutting and lay-up.
  • Expanding honeycomb reinforcement: Heat-cure expansion supports sealing, splicing and reinforcing honeycomb details.

Applications

Applications include sealing, splicing and reinforcing aerospace honeycomb materials.

Product Family

LOCTITE EF562S

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Unsupported expandable epoxy film adhesive
Color
Amber
Density (g)
0.51 g/cm3
Physical Properties
Volatiles
0.14 %