LOCTITE EF562

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

LOCTITE EF562

Main features

  • Foaming Epoxy Film Adhesive
  • Uniform Cell Structure
  • Dual-Cure Bonding Processing

Product Description

LOCTITE® EF 562 AERO (formerly Hysol® MA 562) is a foaming epoxy film adhesive designed for honeycomb core splicing, sealing, and reinforcement applications in aerospace composite structures. The unsupported expandable adhesive cures at either 250°F (121°C) or 350°F (177°C) and develops a uniform closed-cell structure that helps reduce moisture ingress into splice areas. Its low exotherm, excellent slump resistance, and dual-cure capability make it particularly suitable for thick splice sections and co-cure manufacturing processes.

Key Features & Benefits

  • Foaming epoxy film adhesive for aerospace honeycomb structures.
  • Uniform cell structure reduces moisture ingress into splice areas.
  • Dual cure schedules at 250°F (121°C) or 350°F (177°C).
  • Excellent slump resistance during processing.
  • Low exotherm suitable for thick bond lines and co-cure assemblies.
  • Asbestos-free formulation.
  • Qualified to numerous aerospace industry specifications.

Recommended Applications

  • Honeycomb core splicing.
  • Honeycomb edge closeouts.
  • Structural reinforcement of composite core panels.
  • Sealing honeycomb core sections.
  • Co-cure composite panel manufacturing.
Product Family

LOCTITE EF562

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Yellow
Density (g)
0.4 g/cm3

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Expandable Epoxy Film Adhesive — Unsupported film adhesive
Appearance Yellow — Film adhesive
Volatile Content <1 % Typical
Available Thickness 0.050 / 0.100 in 1.3 / 2.5 mm
Form 1 × 2 Sheets ft Approx. 0.3 × 0.6 m
Slump <0.125 in <3.18 mm
Expansion 2 to 3.5× — Original uncured thickness
Exotherm <550 °F 0.200 in thickness
Cured Density 25 to 35 lb/ft³ 0.40 to 0.56 g/cc
Shelf Life 6 months ≤ -18°C storage
Out Time 10 days @ 32°C / 20 days @ 24°C — Maximum exposure time
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Service Temperature Range -55 to +177 °C Continuous service
Cure Schedule 60 min @ 121°C or 177°C — 5-10°F/min heat-up rate
Tube Shear Strength 1200 psi 24°C, cured 121°C
Tube Shear Strength 1150 psi 24°C, cured 177°C
Water Boil Retention 1095 psi 3-day water boil exposure
Skydrol Resistance 1085 psi 7 days @ 68°C
Salt Spray Retention 780 psi 30-day exposure
Flexural Strength 830 psi 24°C, cured 121°C
Flexural Strength 770 psi 24°C, cured 177°C
High Temperature Flexural Strength 540 psi 177°C test temperature

Leading Brands Trust in Our Products and Services