Main features

  • Good dielectric strength
  • Excellent printability
  • Fast UV Cure

Product Description

LOCTITE EDAG PF 455BC E&C is a translucent UV curable acrylate that is formulated as a crossover dielectric and is compatible with other EDAG E&C inks. Mainly used as a dielectric ink.

LOCTITE EDAG PF 455BC is resistant to humidity, has excellent printability and adheres well to both treated and untreated polyester film substrates.  It has good dielectric strength and is compatible for use with ElectroDAG conductive and dielectric polymer thick film inks.  

UV Cure 

  • UV lamp 80Watt/cm or
  • UV lamp 120Watt/cm
Product Family

LOCTITE EDAG PF455BC

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 45 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g)
1,02 g/cm3
Physical Properties
Viscosity
13,500 mPa.s

Additional Information

Recommended UV Cure Condition
UV lamp 80Watt/cm or
UV lamp 120Watt/cm
When applying LOCTITE EDAG PF 455BC E&C as a crossover, two layers of approximately 12 to 15μm each should be applied. Cure both layers at an energy level of 0.5Joule/cm2 to obtain a good inter- coat adhesion between the first and second layer and to obtain a maximum adhesion of the crossover.
When using LOCTITE EDAG PF 455BC E&C as a crossover, be sure to dry the inks printed over it within 5 minutes. Do not let the inks printed over LOCTITE EDAG PF 455BC E&C air dry for extended periods of time.