LOCTITE EDAG PF 407C E&C

Harmonization Code : 32159090 | Printing ink, writing or drawing ink, and other inks, whether or not concentrated or solid, specifically for those classified as other within that category

LOCTITE EDAG PF 407C E&C

Main features

  • Screen printable
  • Extended screen residence time
  • Carbon filled

Product Description

LOCTITE EDAG PF407C E&C polymer thick film is designed for production of low voltage circuitry on polyester film and solvent sensitive substrates such as polycarbonate. It can be used in continuous operating temperatures as high as 105°C and it typically used for printed resistors, membrane touch switches, heating elements, flexible circuits and protection against electrostatic discharge (ESD).

LOCTITE EDAG PF407C E&C is a conductive, screen printable thermoplastic with extended screen residence time over EDAG PF 407A E&C. It has good adhesion and flexible, low temperature drying cycles. This ink works on substrates such as Polyester, Polyimide, Polycarbonate, paper and cardboard.

Drying Cycle

  • 30 minutes @ 90°C or
  • 15 minutes @ 120°C

LOCTITE EDAG PF 407C E&C can be dried immediately after printing.

Product Family

LOCTITE EDAG PF407C

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 30 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids
37 %
Specific Gravity
1.1
Physical Properties
Viscosity
42,500 mPa.s

Additional Information

Optimal Storage : 5 to 30 °C

 

TYPICAL SCREEN PRINTING PROCESS
Recommended Thickness
-Applied dry coating thickness , μm 6 to 10


Emulsion Thickness
-Emulsion Thickness , μm 20 to 40

Recommended Squeegee
-Polyurethane , durometer 70 to 75

Recommended Screen Type
-Monofilament polyester screen, threads/cm 61 to 90
-Stainless steel screen , threads/cm 77 to 110

Printing Equipment Type
-Manual
-Semi-automatic
-High speed reel-to-reel