LOCTITE EDAG PF 407A E&C

Harmonization Code : 32159090 | Printing ink, writing or drawing ink, and other inks, whether or not concentrated or solid, specifically for those classified as other within that category

LOCTITE EDAG PF 407A E&C

Main features

  • Print Contact areas
  • Good screen residence time
  • Carbon filled

Product Description

LOCTITE EDAG PF 407A E&C is a carbon filled ink with inert pigment that can be used to print contact areas on flexible circuits.  

LOCTITE EDAG PF 407A is a screen printable, conductive, carbon filled thermoplastic with good screen residence time that is flexible for low temperature drying cycles.

LOCTITE EDAG PF 407A is typically used for printed resistors, membrane touch switches. keyboards, heating elements, flexible circuits and ESD protection. It can continuously operate at a temperature of 105°C and has been successfully used on Polyester, Polyimide, Polycarbonate, paper and cardboard substrates.

Drying Cycle

  • 30 minutes @ 90°C or
  • 15 minutes @ 120°C
Product Family

LOCTITE EDAG PF407A

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 30 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g)
1,12 g/cm3
Physical Properties
Viscosity
35,000 mPa.s

Additional Information

Optimal Storage : 5 to 30 °C

 

TYPICAL SCREEN PRINTING PROCESS
Recommended Thickness
-Applied dry coating thickness , μm 6 to 10


Emulsion Thickness
-Emulsion Thickness , μm 20 to 40

Recommended Squeegee
-Polyurethane , durometer 70 to 75

Recommended Screen Type
-Monofilament polyester screen, threads/cm 61 to 90
-Stainless steel screen , threads/cm 77 to 110

Printing Equipment Type
-Manual
-Semi-automatic
-High speed reel-to-reel