LOCTITE EDAG 456
Harmonization Code : 32159090 | Printing ink, writing or drawing ink, and other inks, whether or not concentrated or solid, specifically for those classified as other within that category
Main features
- Non conductive
- screen printable
- Thermoformable
Product Description
LOCTITE EDAG 456 is a flexible, thermoformable, non-conductive coating which can be applied by screen printing techniques.
LOCTITE® EDAG 456 is compatible with thermoformable silver ink LOCTITE® ECI 1501 and stretchable silver ink LOCTITE® ECI 1014.
Packaging
Please select Package Type.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Density (g)
1.35 g/cm3
Solids
100 %
Physical Properties
Viscosity
12000 mPa.s