LOCTITE EDAG 1415M

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE EDAG 1415M

Main features

  • Silver-Filled Coating Application
  • Low-Resistance Coating Application
  • No Primer or Topcoat Required

Product Description

LOCTITE® EDAG 1415M E&C is a silver-filled thermoplastic conductive coating developed to provide electromagnetic compatibility (EMC) and EMI shielding protection for electronic equipment enclosures. The coating is compatible with many engineering plastics and delivers low surface resistance, high attenuation performance, and excellent environmental durability without requiring a primer or top coat. It can be applied by spray or brush and air dries rapidly for efficient production processing.

Key Features & Benefits

  • Silver-filled thermoplastic conductive coating.
  • Designed for EMC and EMI shielding applications.
  • Maintains low resistance after environmental exposure.
  • No primer or top coat required.
  • Suitable for spray or brush application.
  • Fast air-dry processing with optional forced drying.
  • Compatible with plastics used in electronic enclosures.

Recommended Applications

  • EMI shielding of plastic electronic housings.
  • EMC compliance coatings.
  • Electronic equipment enclosures.
  • Conductive coating applications requiring low resistance.
  • Industrial electronic assemblies and housings.
Product Family

LOCTITE EDAG 1415M

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Silver
Density
1,630 kg/m3
Solids
58 %
Physical Properties
Viscosity
375 mPa.s
Thermal Properties
Flash Point
14 °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Thermoplastic Conductive Coating — Silver-filled EMC coating
Appearance Silver — As supplied
Solids Content 58 % Typical
Viscosity 375 mPa·s (cP) Brookfield, 20°C, 20 rpm
Density 1,630 kg/m³ Typical
Theoretical Coverage 9 m²/kg 10 μm coating thickness
Shelf Life 18 months 5 to 30°C storage
Flash Point 14 °C Typical
Operating Temperature 105 °C Maximum service temperature
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Recommended Coating Thickness 10 - 15 μm For EMI shielding performance
Attenuation 60 dB 1,000 MHz, 25 μm thickness
Sheet Resistance <0.015 Ω/sq 25 μm coating thickness
Dry to Touch Time 10 minutes Ambient conditions
Handling Time 20 minutes Approximate
Air Dry Time 4 - 8 hours Good coating properties achieved
Recommended Drying Cycle 30 min @ 70-80 °C Forced drying improves conductivity
Spray Pressure 2.0 - 2.5 bar Recommended application setting
Nozzle Diameter 1.0 - 1.5 mm Spray application