LOCTITE ECI1016

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

LOCTITE ECI1016

Main features

  • High-Speed Rotary Screen Printing
  • Low-Resistance Silver Conductive Traces
  • Two-Minute Hot-Air Drying

Product Description

LOCTITE ECI 1016 EC is a low-viscosity, silver-filled thermoplastic conductive ink for high-speed roll-to-roll rotary screen printing. The gray paste contains 68% solids and is formulated for printed antennas and conductive circuits on PET or paper. The recommended hot-air drying cycle is 2 minutes at 150 deg C. After drying, the ink has 5B cross-cut adhesion on untreated PET and sheet resistance of 0.0065 ohm/sq/25 um after 10 minutes at 150 deg C. The dried material has a maximum operating temperature of 105 deg C.

Key features

  • High-speed rotary printing: Low viscosity supports roll-to-roll rotary screen application.
  • Low-resistance silver traces: The dried film reaches 0.0065 ohm/sq/25 um under the documented condition.
  • Rapid hot-air drying: The recommended guideline cycle is 2 minutes at 150 deg C.

Applications

Applications include RFID antennas, printed antennas and conductive circuits on PET or paper.

Product Family

LOCTITE ECI1016

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Gray paste
Density (g)
2.6 g/cm3
Solids
68 %
Physical Properties
Drying Time
2 minutes minutes
Thixotropic index
1.7
Viscosity
7,300 mPa.s

Additional Information

Technical properties

As-supplied properties

Typical values for the undried conductive ink.

Property Value Unit Method / condition
AppearanceGray pasteAs supplied
Filler typeSilverConductive filler
Solids content68%Undried material
Density2.6g/mlUndried material
Viscosity7,300mPa sRheometer, 1.5 s^-1, 25 deg C
Thixotropic index1.715/1.5 s^-1
Theoretical coverage8m^2/kgAt 10 um dry coating thickness
Shelf life365daysAt 2 to 8 deg C
Technical properties

Final-state properties

Typical dried-film properties under the stated conditions.

Property Value Unit Method / condition
Maximum operating temperature105deg CDried material
Adhesion on untreated PET5BgradeCross-cut test
Sheet resistance0.0065ohm/sq/25 um4-point probe after 10 minutes at 150 deg C

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers