LOCTITE ECI 1014 E&C

Harmonization Code : 32159090 | Printing ink, writing or drawing ink, and other inks, whether or not concentrated or solid, specifically for those classified as other within that category

LOCTITE ECI 1014 E&C

Main features

  • Low temperature drying
  • High conductivity
  • Compatible for use with polycarbonate, polyester and polyurethane

Product Description

LOCTITE® ECI 1014 is a highly conductive, silver, high-elongation ink based on a thermoplastic polyurethane binder. This combined stretchability and high conductivity enables the development of medical wearables, smart textiles, automotive interiors, and flexible heater applications.

LOCTITE® ECI 1014 can be dried at temperatures as low as 80°C (176°F). It is suitable for screen printing or high-speed printing after dilution, and compatible with solvent-sensitive substrates such as polycarbonate, polyester or thermoplastic polyurethane.

Drying cycle

  • 15 minutes @ 120°C
Product Family

LOCTITE ECI1014

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 20 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Gray
Density (g)
2.2 g/cm3
Solids
65.4 %
Physical Properties
Thixotropic index
2.0
Viscosity
10,000 mPa.s

Additional Information

DIRECTIONS FOR USE

1. Surface Preparation

  • Clean the surface thoroughly prior to application

2. Mixing/Dilution

  • Mix thoroughly before use to ensure it is homogenous. 
  • Moderate heating of the ink, up to 40°C, can improve product homogeneity
  • Should dilution be necessary use Dowanol DPM (CAS: 34590-94-8). Henkel recommends a maximum of 10 wt%. This should be accomplished by adding solvent at 0.5 wt% intervals by weight until desired viscosity and printability are achieved.

3. Application

  • LOCTITE ECI 1014 E&C may be applied by screen printing method.
  • Recommended screen and printing parameters are:
    Emulsion Thickness, µm: 
      Solvent resistant 10 to 40
    Squeegee Hardness 70 to 90
    Screen Type, Polyester screen, cm 77-48