LOCTITE EA E-40EXP

Main features

  • Self-Leveling Horizontal Potting
  • Controlled 2:1 Metered Mixing
  • Room-Temperature Potting Cure

Product Description

LOCTITE EA E-40EXP is a two-component, self-leveling epoxy potting compound for electric motors and wire-conduit isolation. The white resin and black amine hardener mix at 2:1 by volume to form a black material that flows through horizontal cavities and cures at room temperature. Typical mixed-material values include a gel time below 45 minutes at 22 deg C and a tack-free time of 75 minutes or less. After seven days at 25 deg C, the cured epoxy reaches greater than 80 Shore D hardness and provides 38 kV/mm dielectric breakdown strength.

Key features

  • Self-leveling cavity fill: The mixed epoxy flows into horizontal voids and supports bottom-up potting.
  • Controlled 2:1 mixing: Resin and hardener use a 2:1 volume ratio for cartridge or bulk-metered dispensing.
  • Room-temperature cure: The system cures at room temperature, with heat acceleration up to 93 deg C.

Applications

Applications include potting wire conduits and electrical motor areas where a self-leveling two-component epoxy is specified.

Product Family

LOCTITE EA E-40EXP

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
White liquid / Black liquid
Component System
Two (Resin / Hardener)
Mix Ratio
100 : 45.9
Specific Gravity
1.2 / 1.1
Mechanical Properties
Elongation
4 %
Thermal Properties
Glass Transition Temperature (Tg)
52 °C

Additional Information

Technical properties

As-supplied properties

Resin, hardener and mixed-system values before cure.

Property Value Unit Method / condition
Mix ratio by volume2:1Resin to hardener
Mix ratio by weight100:45.9Resin to hardener
Resin viscosity20,800mPa sBrookfield DV-II, spindle 14, 10 rpm, 25 deg C
Hardener viscosity6,400mPa sBrookfield RVT, spindle 14, 10 rpm, 25 deg C
Mixed specific gravity1.2At 25 deg C
Tack-free time75 or lessminutesMixed material
Gel timeLess than 45minutesAt 22 deg C
Optimal storage8 to 21deg CUnopened container in a dry location
Technical properties

Final-state properties

Typical cured-material values after 7 days at 25 deg C unless otherwise stated.

Property Value Unit Method / condition
Shore hardnessGreater than 80Shore DISO 868; cured 7 days at 25 deg C
Glass transition temperature52deg CASTM E1640; cured 7 days at 25 deg C
Coefficient of thermal expansion26 x 10^-6 pre-Tg; 151 x 10^-6 post-TgK^-1ISO 11359-1
Tensile strength66N/mm^2ISO 527-2; cured 7 days at 25 deg C
Tensile modulus2,750N/mm^2ISO 527-2; cured 7 days at 25 deg C
Elongation4%ISO 527-2; cured 7 days at 25 deg C
Thermal conductivity0.25W/(m K)ASTM E1530; cured 7 days at 25 deg C
Dielectric breakdown strength38kV/mmIEC 60243-1; cured 7 days at 25 deg C