LOCTITE EA E-310

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE EA E-310

Main features

  • Glass, Metal, and Plastic Bonding
  • 6,000 psi Shear Strength
  • Up to 5.1 mm Gap Filling

Product Description

LOCTITE® EA E-310 is a single-component epoxy adhesive for structural bonding of metal, glass, and plastic. The silver-gray material cures at elevated temperatures and has a typical viscosity of 400,000 mPa·s at 25°C, supporting controlled placement and gap filling up to 5.1 mm (0.2 in). The cured adhesive is characterized by vibration and impact resistance, with typical lap shear strength reaching 6,000 psi (41 MPa) on steel under ASTM D1002 testing. Its documented operating-temperature range is -85°C to 204°C (-65°F to 400°F), making it suitable for evaluation in bonded assemblies exposed to a broad range of service temperatures.

Key features

  • Single-component heat-cure epoxy: Eliminates component mixing and cures in 12 to 45 minutes at documented temperatures from 150°C to 200°C.
  • Structural bonding performance: Provides typical ASTM D1002 lap shear strength of 6,000 psi (41 MPa) on steel and 5,800 psi (40 MPa) on aluminum.
  • Gap-filling consistency: The 400,000 mPa·s viscosity at 25°C and maximum documented gap of 5.1 mm support thicker adhesive sections.

Applications / Suitable for

  • Structural bonding of metal substrates
  • Structural bonding of glass
  • Structural bonding of plastic substrates
Product Family

LOCTITE EA E-310

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Silver gray
Specific Gravity
1.5
Physical Properties
Viscosity
400,000 mPa.s
Thermal Properties
Flash Point
93 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the adhesive before elevated-temperature curing.

Property Value Unit Method / condition
Chemical type Epoxy — Single-component material
Appearance Silver-gray — Typical value
Viscosity 400,000 mPa·s (cP) At 25°C
Specific gravity 1.5 — At 25°C
Flash point >93 (>200) °C (°F) TCC
Maximum gap 5.1 (0.2) mm (in) Typical documented maximum

After-processing / final-state properties

Typical properties of the cured adhesive. Strength values are specific to the documented substrates and laboratory test configurations.

Property Value Unit Method / condition
Shear strength 6,000 (41) psi (MPa) ASTM D1002; steel/steel
Shear strength 5,800 (40) psi (MPa) ASTM D1002; aluminum/aluminum
Shear strength 1,800 (12) psi (MPa) ASTM D1002; SMC plastic/SMC plastic; substrate failure
Peel strength 24 lb/linear in ASTM 1876; steel/steel
Operating temperature -85 to 204 (-65 to 400) °C (°F) Typical cured-material property
Glass transition temperature 118 (244) °C (°F) Typical value; test method not stated
Thermal conductivity 0.40 Btu/ft²/hr/°F Typical value
Volume resistivity 3.1 × 106 ohm-cm Typical cured-material property