LOCTITE EA 9845SF

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

LOCTITE EA 9845SF

Main features

  • Co-Cured Composite Surfacing
  • Paint-Ready Surface Quality
  • Reduced Core Crush and Porosity

Product Description

LOCTITE EA 9845SF AERO is an epoxy-based composite surfacing film for co-cured honeycomb-stiffened composite parts. Incorporated with the composite lay-up, the film forms an integrated surface layer intended to improve surface quality and provide a paintable finish after cure. The surfacing layer can help reduce core crush and surface porosity when processed within the required lay-up and cure conditions. Applications include aerospace composite panels and sandwich structures that require an integrated surfacing layer rather than a conventional bonded-joint adhesive.

Key features

  • Co-cured composite surfacing: The epoxy film integrates with compatible composite lay-ups during cure.
  • Paintable surface finish: The cured surfacing layer provides a paintable composite surface.
  • Core and porosity control: The film is used to reduce core crush and surface porosity under the required lay-up and cure conditions.

Applications

Applications include composite surfacing, honeycomb-stiffened panels and co-cured aerospace sandwich structures.

Product Family

LOCTITE EA 9845SF

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Blue
Other Properties
Storage Temperature
≤4 °C