Loctite EA 9837.1 030OST AERO

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Loctite EA 9837.1 030OST AERO

Main features

  • Long-Open-Time Composite Surfacing
  • Fast 121/177 deg C Cure
  • High-Adhesion Composite Surface Film

Product Description

LOCTITE EA 9837.1 AERO is an epoxy-based composite surfacing film designed for aerospace composite structures and honeycomb-stiffened composite parts. Available in 0.030 psf (150 g/m²) and 0.035 psf (170 g/m²) formats, it is engineered to improve surface quality while minimizing core crush and porosity during composite fabrication. The film is co-curable with composite prepregs and supports cure schedules at either 250°F (121°C) or 350°F (177°C). Its paintable surface, resistance to microcracking, and compatibility with lightning strike screens and foils make it suitable for aerospace composite components requiring enhanced surface finish and paint adhesion.

Key features

  • Composite Surfacing Film: Improves the surface quality of honeycomb-stiffened composite parts while minimizing porosity and core crush.
  • Co-Curable Epoxy System: Compatible with composite prepregs and can be cured at either 250°F (121°C) or 350°F (177°C).
  • Paintable Surface Quality: Provides a high-quality paintable surface with greater than 95% primer adhesion in cross-hatch paint adhesion testing.

Applications / Suitable for

  • Honeycomb-stiffened composite structures
  • Aerospace composite parts requiring improved surface finish
  • Composite components requiring paint-ready surfaces
  • Co-cure processing with aerospace prepregs
  • Applications utilizing lightning strike screens and foils
Product Family

LOCTITE EA 9837.1 030OST

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Opaque Gray

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied properties for LOCTITE EA 9837.1 AERO composite surfacing film.

Property Value Unit Method / condition
Color Opaque Gray - Visual examination
Available Weight 150 or 170 g/m² Nominal film weight
Gel Time 20 - 35 minutes At 250°F (121°C)
Gel Time 0.5 - 2 minutes At 350°F (177°C)
Volatiles 1.5 % Maximum typical value
Open Assembly Time At least 21 days 77°F (25°C)
Shelf Life 12 months Stored at 0°F (-18°C) or below
Technical properties

After-processing / final-state properties

Representative cured-system and performance data.

Property Value Unit Method / condition
Primer Adhesion >95 % Initial, no exposure, cross-hatch paint adhesion
Primer Adhesion >95 % After 7 days deionized water exposure at 25°C
Cure Schedule 2 hours 250°F (121°C) cure, 45 psi pressure
Alternative Cure Schedule 1.5 hours 350°F (177°C) cure, 45 psi pressure