LOCTITE EA 9658.060UNS

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

LOCTITE EA 9658.060UNS

Main features

  • Unsupported 0.060 lb/sf Film
  • 177 deg C Cure Capability
  • Extended 15-Day Assembly Window

Product Description

LOCTITE EA 9658.060 PSF UNS AERO is the 0.060 lb/sf unsupported configuration of the high-temperature EA 9658 epoxy film adhesive for nacelle metal, composite and honeycomb bonding. The UNS construction contains no fabric carrier and cures for 1 hour at 177 deg C under maintained pressure. Open assembly time is at least 15 days at 25 deg C or 10 days at 32 deg C, while refrigerated storage at -18 deg C or below provides a 9-month warranty life. Applications include high-temperature aerospace structures requiring the specified unsupported film configuration.

Key features

  • Unsupported film construction: The 0.060 lb/sf UNS configuration contains no fabric carrier.
  • High-temperature cure: The film cures for 1 hour at 177 deg C under maintained pressure.
  • Extended assembly window: Open assembly time is at least 15 days at 25 deg C or 10 days at 32 deg C.

Applications

Applications include nacelle metal, composite and honeycomb bonding where the 0.060 lb/sf unsupported construction is specified.

Product Family

LOCTITE EA 9658.060UNS

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Other Properties
Storage Temperature
≤ -18 °C °C
General Properties
Density
0.72 kg/m3

Additional Information

Technical properties

As-supplied properties

Configuration-specific and common family handling values.

Property Value Unit Method / condition
ConfigurationEA 9658 .060 PSF UNSSpecific product variant
ConstructionUnsupported adhesiveNo fabric carrier
Standard package36 in x 150 ft450 sf roll
Open assembly timeAt least 15daysAt 25 deg C
Open assembly timeAt least 10daysAt 32 deg C
Storage temperature-18 or belowdeg CSealed container
Warranty life9monthsAt -18 deg C or below, from shipment
Cure schedule1 hour at 177 deg CHeat-up rate 2.2 to 4 deg C/minute