Loctite EA 9392 AERO Epoxy Adhesive

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Loctite EA 9392 AERO Epoxy Adhesive

Main features

  • 1,000 psi Aluminum Lap Shear
  • Thixotropic Gap-Filling Control
  • 75-Minute Working Window

Product Description

LOCTITE® EA 9392 AERO Epoxy Paste Adhesive is a two-component, room-temperature-curing epoxy paste adhesive for durable bonded assemblies. The thixotropic material supports gap-filling and potting applications while remaining workable for 75 minutes at 77°F/25°C when evaluated as a 100 g mass. It develops handling strength after 24 hours at 77°F/25°C and may be fully cured at room temperature or with an accelerated thermal schedule. Testing on prepared 2024-T3 aluminum demonstrates tensile lap shear performance across temperatures from -67°F/-55°C to 350°F/177°C, with 1,000 psi/6.9 MPa retained at the upper test temperature.

Key features

  • Elevated-temperature shear performance: Retains 1,000 psi/6.9 MPa tensile lap shear strength at 350°F/177°C under ASTM D1002 test conditions.
  • Thixotropic epoxy paste: Supports gap filling and potting while limiting uncontrolled flow during application.
  • Flexible cure scheduling: Cures in 5–7 days at 77°F/25°C or in 1 hour at 180°F/82°C for small adhesive masses.

Applications / Suitable for

  • Bonded assemblies requiring room-temperature cure
  • Gap-filling adhesive applications
  • Potting applications
  • Applications evaluated for shear strength at elevated temperatures
Product Family

LOCTITE EA 9392

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
Viscosity (Part A)
420,000 mPa.s
Viscosity (Part B)
660,000 mPa.s
General Properties
Mix Ratio
100:32

Additional Information

Technical properties

As-supplied / before-processing properties

Typical component, mixed-material and processing properties. Component identities and test conditions are retained where relevant.

Property Value Unit Method / condition
Product type Two-component epoxy paste adhesive — As supplied
Rheology Thixotropic — Uncured material
Color — Part A Gray — Visual
Color — Part B Amber — Visual
Color — mixed Gray — After mixing Parts A and B
Viscosity — Part A 4,200 Poise 77°F; Brookfield HBT, spindle 7 at 20 rpm
Viscosity — Part A 420 Pa·s 25°C; Brookfield HBT, spindle 7 at 2.1 rad/s
Viscosity — Part B 6,600 Poise 77°F; Brookfield HBT, T-bar C at 5 rpm
Viscosity — Part B 660 Pa·s 25°C; Brookfield HBT, spindle 6 at 0.5 rad/s
Density — Part A 1.37 g/ml Uncured component
Density — Part B 1.0 g/ml Uncured component
Density — mixed 1.29 g/ml Parts A and B combined
Mix ratio by weight — Part A : Part B 100 : 32 parts Weight basis
Mix ratio by volume — Part A : Part B 100 : 44 parts Volume measurement is not recommended for structural applications unless ratio-control precautions are used
Pot life 75 minutes 100 g mass at 77°F/25°C; ASTM D2471 in water bath
Handling-strength time 24 hours At 77°F/25°C; full bond strength has not yet developed
Room-temperature cure 5–7 days At 77°F/25°C for normal performance
Accelerated complete cure 1 hour At 180°F/82°C; small masses only
Maximum stated accelerated-cure temperature 200 / 93 °F / °C Accelerated curing; small masses only
Maximum recommended mixed quantity 450 g Do not mix larger quantities because dangerous exothermic heat buildup may occur
Shelf life — Part A 1 year Stored below 40°F/4°C
Shelf life — Part B 1 year Stored below 40°F/4°C
Shelf life — Part A 1 year Stored below 77°F/25°C
Shelf life — Part B 1 year Stored below 77°F/25°C
Technical properties

After-processing / final-state properties

Typical cured adhesive and bonded-joint results. Cure schedule, substrate preparation, test temperature and test method are retained because they materially affect interpretation.

Property Value Unit Method / condition
Tensile lap shear strength at -67°F/-55°C 3,500 / 24.1 psi / MPa ASTM D1002; 2024-T3 bare PAA aluminum; cured 5 days at 77°F/25°C
Tensile lap shear strength at 77°F/25°C 4,300 / 29.6 psi / MPa ASTM D1002; 2024-T3 bare PAA aluminum; cured 5 days at 77°F/25°C
Tensile lap shear strength at 180°F/82°C 2,500 / 17.2 psi / MPa ASTM D1002; 2024-T3 bare PAA aluminum; cured 5 days at 77°F/25°C
Tensile lap shear strength at 250°F/121°C 2,000 / 13.8 psi / MPa ASTM D1002; 2024-T3 bare PAA aluminum; cured 5 days at 77°F/25°C
Tensile lap shear strength at 300°F/149°C 1,300 / 9.0 psi / MPa ASTM D1002; 2024-T3 bare PAA aluminum; cured 5 days at 77°F/25°C
Tensile lap shear strength at 350°F/177°C 1,000 / 6.9 psi / MPa ASTM D1002; 2024-T3 bare PAA aluminum; cured 5 days at 77°F/25°C
Blister shear strength at -67°F/-55°C 3,000 / 20.7 psi / MPa ASTM D3165; 2024-T3 bare FPL-etched aluminum; cured 7 days at 77°F/25°C
Blister shear strength at 77°F/25°C 4,000 / 27.6 psi / MPa ASTM D3165; 2024-T3 bare FPL-etched aluminum; cured 7 days at 77°F/25°C
Blister shear strength at 180°F/82°C 2,500 / 17.2 psi / MPa ASTM D3165; 2024-T3 bare FPL-etched aluminum; cured 7 days at 77°F/25°C
Blister shear strength at 250°F/121°C 2,000 / 13.8 psi / MPa ASTM D3165; 2024-T3 bare FPL-etched aluminum; cured 7 days at 77°F/25°C
Blister shear strength at 300°F/149°C 1,000 / 6.9 psi / MPa ASTM D3165; 2024-T3 bare FPL-etched aluminum; cured 7 days at 77°F/25°C
T-peel strength at 77°F/25°C 20 / 89 lb/in / N/25 mm ASTM D1876; 2024-T3 bare PAA aluminum; cured 5 days at 77°F/25°C
Bell peel strength at 77°F/25°C 40 / 178 lb/in / N/25 mm ASTM D1876; 2024-T3 bare PAA aluminum; cured 7 days at 77°F/25°C
Bell peel strength at 180°F/82°C 30 / 133 lb/in / N/25 mm ASTM D1876; 2024-T3 bare PAA aluminum; cured 7 days at 77°F/25°C
Service temperature based on retained lap shear Approximately 350 / 177 °F / °C Defined as the temperature at which 1,000 psi/6.9 MPa is retained under ASTM D1002
Tensile strength at 77°F/25°C 6,000 / 41.3 psi / MPa ASTM D638; 0.125 in/3.18 mm cast specimen
Tensile modulus at 77°F/25°C 475 / 3,273 ksi / MPa ASTM D638; 0.125 in/3.18 mm cast specimen
Elongation at break at 77°F/25°C 4 % ASTM D638; 0.125 in/3.18 mm cast specimen
Glass-transition temperature — dry 164 / 73 °F / °C Cured 7 days at 77°F/25°C
Glass-transition temperature — wet 144 / 62 °F / °C Cured 7 days at 77°F/25°C; immersed in 77°F/25°C water until equilibrium
Glass-transition temperature — dry, accelerated cure 356 / 180 °F / °C Cured 1 hour at 180°F/82°C
Compressive strength at 2% offset 9,300 / 64.1 psi / MPa ASTM D695 at 77°F/25°C; 1.15 in/29.2 mm diameter × 1 in/25.4 mm cylindrical specimens; cured 7 days at 77°F/25°C